==TPT Wire Bonder==
=TPT HB100 Wire Bonder =
Wire bonding is a method of making interconnections between a microchip and other electronics as part of semiconductor device fabrication. The TPT HB100 Wire Bonder was bought in 2025. It is an automatic desktop wire bonder and supports process guidance for the user. The bonder allows wedge- and ball-bonding, ribbon- and bump-bonding with one bond head.


[[Image:TPTWireBonder.jpg|300x300px|thumb|TPT Wire Bonder Building 346, 2nd floor]]
'''The user manual(s), user APV(s), technical information and contact information can be found in LabManager (requires login):'''
<div style="border:1px solid #cccccc; padding:10px; background:#f9f9f9;">


Wire bonding is a method of making interconnections between a microchip and other electronics as part of semiconductor device fabrication. The TPT-H05 is a manuel wire bonder.
'''Related Page:'''


[[/TPT HB 100 wire bonder: process details| TPT HB 100 wire bonder: process details]]
</div>
[https://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=533 TPT HB100 Wire Bonder]


#Wedge Bonding
=Ball Wire Bonder K&S 4524=
:Gold wire 25 my wire.
<!-- copyright issue kabi - replace with actual photo and numbering
:Alluminium wire 25 my wire.
[[Image:K&S_4524_ball_wire-bonder.jpg|300x300px|thumb|The Ball Wire Bonder K&S 4524, <br/> Packlab, Building 347, 1st floor]]
:Min. bonding area 200 my.
-->


#Ball bonding
[[Image:K-S 4524 wirebonder DTU.jpg|thumb|200px|K&S 4524 ball wire bonder]]
:Ball bonding gives free choice of  bonding direction. First bond forms a small ball and second bond is a wedge bond.


:Gold only 25 my wire.
<span style="background:#FF2800">The bonder is currently in building 346 Phoenex lab.</span>
:Min. bonding pad 300 my.
 
:Sample withstand heating to 120 degree C.
The Ball Wire Bonder K&S 4524 is for high precision ball bonding. It is a semi-automatic wire bonder with good control of bond placement and bonding parameters.
 
'''The user manual(s), user APV(s), technical information and contact information can be found in LabManager (requires login):'''
 
[http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=307 Ball Wire Bonder]
<br clear=all>
 
=Equipment performance and process related parameters=
 
[[Image:single wire bonding.jpg|300px|thumb|left|Ball wire bond]]
<br clear=all>
 
{| border="2" cellspacing="0" cellpadding="2"
 
!border="none" style="background:silver; color:black;" align="center"|Equipment
|style="background:WhiteSmoke; color:black"|<b>TPT HB100 Wire Bonder</b>
|style="background:WhiteSmoke; color:black"|<b>Ball Wire Bonder K&S 4524</b>
|-
!style="background:silver; color:black;" align="center" width="60"|Purpose
|style="background:WhiteSmoke; color:black"|
*Al and Au 25µm wire bonding
*Wedge and ball wire bonding
* Au ribbon (100x20µm) bonding<br />
|style="background:WhiteSmoke; color:black"|
*Au 25µm wire bonding
*Ball wire bonding
|-
!style="background:silver; color:black;" align="center" width="60"|Performance
|style="background:WhiteSmoke; color:black"|
*Manual operation
*Wedge bonding:
**recommended min. bonding area 200 µm x 200 µm
*Ball bonding:
**recommended min. bonding area 200 µm x 200 µm
**recommended temperature 120 <sup>o</sup>C.
|style="background:WhiteSmoke; color:black"|
*Semi-automatic and manual operation
*Bond placement laser pointer
*recommended min. bonding area 100 µm x 100 µm
*recommended temperature 120 <sup>o</sup>C.
|-
!style="background:silver; color:black" align="center" valign="center"|Substrates
|colspan="2" style="background:WhiteSmoke; color:black"|
*Should be able to withstand the wire bonding temperature
*Typical materials are: Alumina (Al2O3), AluminumNitride (AlN), std. circuit boards (FR4)
|-
|}
 
<br clear="all" />

Latest revision as of 10:59, 24 September 2026

TPT HB100 Wire Bonder

Wire bonding is a method of making interconnections between a microchip and other electronics as part of semiconductor device fabrication. The TPT HB100 Wire Bonder was bought in 2025. It is an automatic desktop wire bonder and supports process guidance for the user. The bonder allows wedge- and ball-bonding, ribbon- and bump-bonding with one bond head.

The user manual(s), user APV(s), technical information and contact information can be found in LabManager (requires login):

TPT HB100 Wire Bonder

Ball Wire Bonder K&S 4524

K&S 4524 ball wire bonder

The bonder is currently in building 346 Phoenex lab.

The Ball Wire Bonder K&S 4524 is for high precision ball bonding. It is a semi-automatic wire bonder with good control of bond placement and bonding parameters.

The user manual(s), user APV(s), technical information and contact information can be found in LabManager (requires login):

Ball Wire Bonder

Equipment performance and process related parameters

Ball wire bond


Equipment TPT HB100 Wire Bonder Ball Wire Bonder K&S 4524
Purpose
  • Al and Au 25µm wire bonding
  • Wedge and ball wire bonding
  • Au ribbon (100x20µm) bonding
  • Au 25µm wire bonding
  • Ball wire bonding
Performance
  • Manual operation
  • Wedge bonding:
    • recommended min. bonding area 200 µm x 200 µm
  • Ball bonding:
    • recommended min. bonding area 200 µm x 200 µm
    • recommended temperature 120 oC.
  • Semi-automatic and manual operation
  • Bond placement laser pointer
  • recommended min. bonding area 100 µm x 100 µm
  • recommended temperature 120 oC.
Substrates
  • Should be able to withstand the wire bonding temperature
  • Typical materials are: Alumina (Al2O3), AluminumNitride (AlN), std. circuit boards (FR4)