Jump to content

LabAdviser/314/Preparation 314-307/Others: Difference between revisions

Jenk (talk | contribs)
Created page with "<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>200px '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu...."
 
Jenk (talk | contribs)
mNo edit summary
 
(18 intermediate revisions by 3 users not shown)
Line 1: Line 1:
<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>[[image:Under_construction.png|200px]]


'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/LabAdviser/314/Preparation_314-307/Others click here]'''
{{cc-nanolab}}
[[Category:314]]
[[Category:314-Preparation]]
= Sonicators =
<!-- == Ultrasonic Branson 2510 ==
Operating Manual: [https://store-19uyxzz.mybigcommerce.com/content/Branson/B_SeriesManual.pdf  Brochure] or [[:File:Branson Ultrasonic Cleaner 2510 Operating manual.pdf]]
[[File:IMG_3676.JPG|250px|left|thumb|Location at DTU Nanolab Building 307, Room 109]]<br />
<br clear="all" />
-->
== VWR Ultrasonic Cleaner ==
[http://www.massetrecovery.com/pictures12/VWR%20Ultrasonic%20cleaner.pdf  Brochure]
[[File:IMG_3678.JPG|250px|left|thumb|Location Building 314, Common Area]]<br />
<br clear="all" />
= Hot plates =
== Nuova hot plate ==
[http://www.laboratory-equipment.com/laboratory-equipment/nuova-hot-plates-stirrers.php  Brochure]
[[File:IMG_3672.JPG|250px|left|thumb|Location at DTU Nanolab Building 307, Room 109]]<br />
<br clear="all" />
== Hot plate Prep Room1 ==
= Plasma cleaner & Pumping Station =
== Fischione Plasma Cleaner model 1020 ==
The Plasma Cleaner automatically and quickly removes organic contamination (hydrocarbon) from electron microscopy specimens and specimen holders. A low energy, reactive gas plasma cleans without changing the specimen’s elemental composition or structural characteristics. The Plasma Cleaner features easy-to-use front panel controls and an oil-free vacuum system for optimal processing.
[http://www.fischione.com/products/contamination-solutions/model-1020-plasma-cleaner Brochure]
[[File:IMG_3682.JPG|250px|left|thumb|Location Building 307, Prep Room 03]].<br />
<br clear="all" />
== Pumping Cube for single TEM specimen holder ==
This pumping cube is mainly used to check vacuum tightness of home made TEM holders. It is running a turbo pump, which can evacuate the chamber down to about 10<sup>-7</sup> mbar. The pressure is measured by a wide-range gauge and recorded in a Labview program.
[[File:IMG_3663.JPG|300px|left|thumb|Location Building 307, behind Room 111 (T12 TEM)]]<br />
<br clear="all" />


'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/LabAdviser/314/Preparation_314-307/Others click here]'''
== Gatan Turbo Pumping Station model 655 ==
 
Capacity: 4 specimen holders. The turbo pumping station is a completely self-contained, compact, benchtop pumping station designed to regenerate the sorb material in cooling and cryo-transfer holder dewars and for vacuum storage of transmission electron microscope (TEM) holders or samples.
 
REMEMBER: When removing a holder, all other holder tubes are vented as well. Check, if one of the cryo-holder dewars is connected for pumping and running a pumping cycle (zeolite cycle). If this is the case, don't remove a holder. Get in contact with the cryo-holder user. There should be a note at the pumping station. When the zeolite cycle is finished, close the valves to the dewar before removing a holder.
[http://www.gatan.com/products/tem-specimen-holders/turbo-pumping-station/ Brochure]
[[File:IMG_3677.JPG|250px|left|thumb|Location Building 314, Prep Room 03]]<br />
<br clear="all" />
 
= Vacuum Pick-Up System =
[[File:Vacuum Pick-Up System.jpg|250px|left|thumb|Location at DTU Nanolab Building 307, Room 109]]<br />