For this exposure we coated a 100 mm Si wafer with 70 nm ZEP 520A resist. To hit the relatively small feature size it is essential to work with a thin resist layer. | For this exposure we coated a 100 mm Si wafer with 70 nm ZEP 520A resist. To hit the relatively small feature size it is essential to work with a thin resist layer. | ||
The exposure was done on our state of the art JEOL 9500 FSZ exposure system. If you are interested in seeing the system in operation consider this video on our Youtube channel. Exposure was done at a low beam current of only 0.22 nA and a voltage of 100 keV. The DTU logo on the chip was however exposed at a much higher beam current. | The exposure was done on our state of the art JEOL 9500 FSZ exposure system. If you are interested in seeing the system in operation consider [https://youtu.be/2bFUO201DS4?si=1GJKJLrZCRnwPmRq this video on our Youtube channel]. Exposure was done at a low beam current of only 0.22 nA and a voltage of 100 keV. The DTU logo on the chip was however exposed at a much higher beam current. | ||
{| style="border: none; border-spacing: 0; margin: 1em auto; text-align: center;" | {| style="border: none; border-spacing: 0; margin: 1em auto; text-align: center;" | ||
| Line 71: | Line 71: | ||
| colspan="1" style="text-align:center;| | | colspan="1" style="text-align:center;| | ||
SEM image of a small fraction of the book. Letter line width is 31 nm and letter height is about 116 nm. | SEM image of a small fraction of the book. Letter line width is 31 nm and letter height is about 116 nm. | ||
|} | |||
The entire book is available for download as a [https://drive.google.com/file/d/10Qa4RgFeogYEqRzbjccWhI5WEIbZZIhM/view?usp=share_link 2.4 gigapixel composite SEM image] viewable in PureRef. | |||
{| style="border: none; border-spacing: 0; margin: 1em auto; text-align: center;" | |||
|- | |||
| [[File:MobyDickTotal.png|400px]] | |||
|- | |||
| colspan="1" style="text-align:center;| | |||
Composite SEM image of the entire book. | |||
|} | |} | ||