Line 11: Line 11:


====For adjusting measurement recipes====
====For adjusting measurement recipes====
To adjust the measurement recipes you need to use the XRDMP Creator mentioned above. This can be found on the support computer right on the instrument apart from being installed on your own computer (see link above for download instructions). Please ask responsible staff for instruction before you start using it on your own. Notice that if you need ''fluorescence suppression'' in your program, for now you need to use the version of XRDMP Creator on the support computer next to the XRD.  
To adjust the measurement recipes you need to use the XRDMP Creator mentioned above. This can be found on the support computer across the hallway in room 904 and can also be installed on your own computer (see link above for download instructions, as it comes bundled with DataViewer). Please ask responsible staff for instruction before you start using it on your own.  
Notice that you need the newest version (from 2026) for transmission measurement setup. This is also what you will find in the link.


====For data analysis====
====For data analysis====

Latest revision as of 12:24, 28 April 2026

Feedback to this page: click here

Unless otherwise stated, this page is written by DTU Nanolab internal


Software for the XRD Powder

For data export

The DataViewer software is a basic program from Malvern Panalytical that accompanies the XRD Powder and allows you to view your measurement results, do simple operations, and export to other formats, e.g., csv or txt. To install DataViewer, please see this document in LabManager - requires login.

For adjusting measurement recipes

To adjust the measurement recipes you need to use the XRDMP Creator mentioned above. This can be found on the support computer across the hallway in room 904 and can also be installed on your own computer (see link above for download instructions, as it comes bundled with DataViewer). Please ask responsible staff for instruction before you start using it on your own. Notice that you need the newest version (from 2026) for transmission measurement setup. This is also what you will find in the link.

For data analysis

We have a license for the software "HighScore" for Rietveld refinement, allowing quantification of the phase composition. For more info about this software including how to access it remotely click here.

You can also use the software from the Rigaku SmartLab XRD to analyse data from the XRD powder. Read about this here.

How to download individual files with reference spectra from the Inorganic Crystal Structure Database (ICSD) (for DTU users and others with access to the ICSD).

Additional software for measurements in a heated atmosphere

If you are going to make measurements in a heated N2 atmosphere, you will need the Nambicon software to control the heater. Download is described in the same document as for DataViewer and XRDMP Creator - requires login.