Specific Process Knowledge/Lithography/Resist/UVresist/exposureDoseNaOH: Difference between revisions
Created page with "The exposure doses listed below are for ''generic'' good exposure results, and can be a compromise between getting good lines, as well as good dots, in both clear field and dark field exposures. The optimal dose for any given specific project, could be different from the listed values. All doses are for standard silicon wafers, unless otherwise stated. Development is done using AZ 351B developer (NaOH) diluted 1:5. ===Aligner: MA6-1=== The Aligner: MA6-1 has an i-line..." |
No edit summary |
||
| (2 intermediate revisions by the same user not shown) | |||
| Line 1: | Line 1: | ||
{{cc-nanolab}} | |||
=Exposure dose when using AZ 351B as developer= | |||
The exposure doses listed below are for ''generic'' good exposure results, and can be a compromise between getting good lines, as well as good dots, in both clear field and dark field exposures. The optimal dose for any given specific project, could be different from the listed values. | The exposure doses listed below are for ''generic'' good exposure results, and can be a compromise between getting good lines, as well as good dots, in both clear field and dark field exposures. The optimal dose for any given specific project, could be different from the listed values. | ||
| Line 4: | Line 7: | ||
==Aligner: MA6-1== | |||
The Aligner: MA6-1 has an i-line notch filter installed. This produces an exposure light peak around 365 nm with a FWHM of 7 nm. | The Aligner: MA6-1 has an i-line notch filter installed. This produces an exposure light peak around 365 nm with a FWHM of 7 nm. | ||
Latest revision as of 13:27, 20 April 2026
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Exposure dose when using AZ 351B as developer
The exposure doses listed below are for generic good exposure results, and can be a compromise between getting good lines, as well as good dots, in both clear field and dark field exposures. The optimal dose for any given specific project, could be different from the listed values.
All doses are for standard silicon wafers, unless otherwise stated. Development is done using AZ 351B developer (NaOH) diluted 1:5.
Aligner: MA6-1
The Aligner: MA6-1 has an i-line notch filter installed. This produces an exposure light peak around 365 nm with a FWHM of 7 nm.
Quality control
Please note that the values listed in the table are not routinely tested as part of quality control.
| Date | Operator | Film thickness | Exposure mode | Dose | Resolution | Comments | |
|---|---|---|---|---|---|---|---|
| AZ 5214E | Long ago | ? | 1.5 µm | ? | 70 mJ/cm2 | ? µm | Not under regular quality control Development: 60 s submersion |
| AZ 5214E | Long ago | ? | 2.2 µm | ? | 72 mJ/cm2 | ? µm | Not under regular quality control Development: 70 s submersion |
| AZ 5214E | Long ago | ? | 4.2 µm | ? | 160 mJ/cm2 | ? µm | Not under regular quality control Development: 180 s submersion |
| AZ 5214E Image reversal |
Long ago | ? | 1.5 µm | ? | 30 mJ/cm2 | ? µm | Not under regular quality control Reversal bake: 100 s @ 110°C Flood exposure: 210 mJ/cm2 Development: 60 s submersion |
| AZ 5214E Image reversal |
Long ago | ? | 2.2 µm | ? | 35 mJ/cm2 | ? µm | Not under regular quality control Reversal bake: 100 s @ 110°C Flood exposure: 210 mJ/cm2 Development: 70 s submersion |
| AZ 4562 | Long ago | ? | 10 µm | ? | 320 mJ/cm2 | ? µm | Not under regular quality control Priming: HMDS Rehydration after SB: none Exposure: Multiple exposures with 15 s pauses is recommended Degassing after exposure: none Development: 300 s submersion |
New resists version in 2023