Specific Process Knowledge/Lithography/Resist/UVresist/exposureDoseMaskAligners: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| (2 intermediate revisions by the same user not shown) | |||
| Line 1: | Line 1: | ||
{{cc-nanolab}} | |||
=Exposure dose for mask aligners= | |||
The exposure doses listed below are for ''generic'' good exposure results, and can be a compromise between getting good lines, as well as good dots, in both clear field and dark field exposures. The optimal dose for any given specific project, could be different from the listed values. | The exposure doses listed below are for ''generic'' good exposure results, and can be a compromise between getting good lines, as well as good dots, in both clear field and dark field exposures. The optimal dose for any given specific project, could be different from the listed values. | ||
| Line 4: | Line 7: | ||
==Aligner: MA6-1== | |||
The Aligner: MA6-1 has an i-line notch filter installed. This produces an exposure light peak around 365 nm with a FWHM of 7 nm. | The Aligner: MA6-1 has an i-line notch filter installed. This produces an exposure light peak around 365 nm with a FWHM of 7 nm. | ||
| Line 47: | Line 50: | ||
<br clear="all" /> | <br clear="all" /> | ||
==Aligner: MA6-2== | |||
The Aligner: MA6-2 has an i-line notch filter installed. This produces an exposure light peak around 365 nm with a FWHM of 7 nm. | The Aligner: MA6-2 has an i-line notch filter installed. This produces an exposure light peak around 365 nm with a FWHM of 7 nm. | ||