{{:Specific Process Knowledge/Lithography/authors_generic}}
{{cc-nanolab}}


'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Lithography/Coaters/Spin_Coater:_Gamma_UV_processing click here]'''
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Lithography/Coaters/Spin_Coater:_Gamma_UV_processing click here]'''
Line 362: Line 362:
|taran
|taran
|4" wafer, no HMDS. 9 points on one wafer, exclusion zone 5mm
|4" wafer, no HMDS. 9 points on one wafer, exclusion zone 5mm
|-
|-style="background:WhiteSmoke; color:black"
|Silicon with native oxide
|4.24 µm
|0.5%
|7/1 2025
|taran
|Old sequence (proximity bake and only 60s by mistake).
4" wafer, with HMDS. 9 points on one wafer, exclusion zone 5mm
|-
|-style="background:WhiteSmoke; color:black"
|Silicon with native oxide
|3.99 µm
|0.3%
|7/1 2025
|taran
|New sequence with contact bake.
4" wafer, with HMDS. 9 points on one wafer, exclusion zone 5mm
|}
|}


==AZ nLOF 2020 coating==
==AZ nLOF 2020 coating==