Specific Process Knowledge/Characterization/XPS/Processing: Difference between revisions
Appearance
No edit summary |
|||
| (6 intermediate revisions by the same user not shown) | |||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Characterization/XPS/Processing click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Characterization/XPS/Processing click here]''' | ||
<!-- Page reviewed 8/5-2023 jmli --> | |||
<!--Checked for updates on 9/5-2023 - ok/jmli --> | |||
<!--Checked for updates on 5/2-2026 - ok/jmli --> | |||
{{Contentbydryetch}} | |||
= XPS Data processing with Avantage = | = XPS Data processing with Avantage = | ||
| Line 28: | Line 34: | ||
=== Guidelines on data processing === | === Guidelines on data processing === | ||
Click [[Specific Process Knowledge/Characterization/XPS/Processing/Guidelines|'''HERE''']] to see some general guidelines on data processing in Avantage. | Click [[Specific Process Knowledge/Characterization/XPS/Processing/Guidelines|'''HERE''']] to see some general guidelines on data processing in Avantage. | ||
== Introduction to data analysis with Avantage by Thermofisher == | |||
In the Youtube video below, the application specialist from Thermorfisher Paul Mack walks you through Avantage...somewhat slowly.. | |||
[https://www.youtube.com/watch?v=gVzYThRKjYQ '''Click here '''] | |||
== Examples of data analysis == | == Examples of data analysis == | ||
| Line 41: | Line 53: | ||
= XPS data analysis with CasaXPS = | = XPS data analysis with CasaXPS = | ||
CasaXPS has its own [https://www.youtube.com/channel/UCUqLBeW-UAjXC55HbRYOabQ Youtube channel] with more than 250 videos so it would be a complete waste of time to make any instructions here. | CasaXPS has its own [https://www.youtube.com/channel/UCUqLBeW-UAjXC55HbRYOabQ Youtube channel] with more than 250 videos so it would be a complete waste of time to make any instructions here. Instead, this is where you as a CasaXPS user could contribute to this database: In case you found any Youtube video that was particularly good, please notify us and we will post a link. | ||
In order to use CasaXPS, you will need to export the data from Avantage and convert it into the Vamas format. | In order to use CasaXPS, you will need to export the data from Avantage and convert it into the Vamas format. Click [[Specific Process Knowledge/Characterization/XPS/Export2CasaXPS | ''this link'']] to find more information. | ||