Jump to content

Specific Process Knowledge/Polymer Processing: Difference between revisions

Mmat (talk | contribs)
mNo edit summary
Clhn (talk | contribs)
mNo edit summary
 
(8 intermediate revisions by one other user not shown)
Line 7: Line 7:
= Polymer Processing =
= Polymer Processing =


There is a wide range of methods available to structure and modify polymers. Some of those are commonly done outside of a cleanroom, in either a standard lab or semi-cleanroom.
There is a wide range of methods available to structure and modify polymers, though commonly done outside of a cleanroom.
 
Many polymer processing methods may require a mask or stamp or some kind, f.ex. injection molding, hot embossing or nano imprint lithography. Some methods can be used to directly "write" into the material, f.ex. laser ablation or micromilling. Other methods, like 3D printing or 2-photon polymerization are called additive methods as they create the structure by a building up the polymer structure.
Many polymer processing methods may require a mask or stamp or some kind, f.ex. injection molding, hot embossing or nano imprint lithography. Some methods can be used to directly "write" into the material, f.ex. laser ablation or micromilling. Other methods, like 3D printing or 2-photon polymerization are called additive methods as they create the structure by a building up the polymer structure.
<br>
<br>
Line 14: Line 15:
* [[Specific Process Knowledge/Lithography/NanoImprintLithography|Nano Imprint Lithography]]
* [[Specific Process Knowledge/Lithography/NanoImprintLithography|Nano Imprint Lithography]]
* [[Specific_Process_Knowledge/Back-end_processing/Hot_Embosser|Hot Embossing]] (Compression Molding)
* [[Specific_Process_Knowledge/Back-end_processing/Hot_Embosser|Hot Embossing]] (Compression Molding)
* [[Specific Process Knowledge/Back-end processing/Polymer Injection Molder|Polymer Injection Molding]] ''(not availabe at DTU Nanolab anymore (moved to DTU Mech))''
* [[Specific Process Knowledge/Back-end processing/Polymer Injection Molder|Polymer Injection Molding]] ''(moved to DTU Construct))''
* Polymer Casting (e.g. PDMS)
* Polymer Casting (e.g. [[Specific Process Knowledge/Characterization/Sample preparation| PDMS Casting]])


'''Special Processes:'''
 
* UV Lithography
 
'''Specialized Processes:'''
* [[Specific Process Knowledge/Lithography/UVLithography|UV Lithography]]
* Additive Techniques
* Additive Techniques
:* 3D printing
:* 3D printing
:* 2-Photon Polymerization Lithography
:* 2-Photon Polymerization Lithography
* Plasma Etching
* Plasma Etching
* FDTS coating (MVD)
* [[Specific Process Knowledge/Thin film deposition/MVD|FDTS coating (MVD)]]
* Laser Ablation
* [[Specific Process Knowledge/Back-end processing/Laser Micromachining Tool|Laser Ablation/Milling]]
* Micro Milling ''(not generally availabe at DTU Nanolab)''
* Micro Milling ''(not generally availabe at DTU Nanolab)''
* Extrusion Coating ''(not availabe at DTU Nanolab)''
* Extrusion Coating ''(not availabe at DTU Nanolab)''
<br>
<br>
<br>
 
== Choose Material for Polymer Processing==
== Choose Material for Polymer Processing==
* Epoxy, e.g. SU-8
* Epoxy, e.g. SU-8
* Thermoplastic, e.g. PMMA, Topas (COC), PS, PC, PP, PET, etc
* Thermoplastic, e.g. PMMA, Topas (COC), PS, PC, PP, PET, etc
* Photo Resist, e.g. AZ resists
* Photo Resist, e.g. AZ resists