Jump to content

Specific Process Knowledge/Etch/DryEtchProcessing/OES: Difference between revisions

Jmli (talk | contribs)
No edit summary
Jmli (talk | contribs)
No edit summary
 
(2 intermediate revisions by the same user not shown)
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/DRIE-Pegasus/nanoetch click here]'''
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/DRIE-Pegasus/nanoetch click here]'''
<!--Checked for updates on 14/5-2018 - ok/jmli -->
<!--Checked for updates on 14/5-2018 - ok/jmli -->
 
<!--Page reviewed by jmli 9/8-2022  -->
<!--Checked for updates on 21/10-2025. ok/ jmli-->


== Optical Endpoint detection systems ==
== Optical Endpoint detection systems ==
{{Template:Contentbydryetch}}
<!--Checked for updates on 3/2-2023 - ok/jmli -->
   
   
During a process, the plasma dissociates the gas molecules present in the process chamber into reactive species that emit light at certain wavelengths. This means that the light coming from the process chamber will be a spectrum in which elements of both process gases and process reactants are found. By analyzing the spectrum we can keep track of when certain species change concentration, i.e. when, for instance, the etch of a thin layer is complete. This is the end point of the etch hence the name.
During a process, the plasma dissociates the gas molecules present in the process chamber into reactive species that emit light at certain wavelengths. This means that the light coming from the process chamber will be a spectrum in which elements of both process gases and process reactants are found. By analyzing the spectrum we can keep track of when certain species change concentration, i.e. when, for instance, the etch of a thin layer is complete. This is the end point of the etch hence the name.