== Overview of the processing options on the XPS Nexsa== | == Overview of the processing options on the XPS Nexsa== | ||
The acquisition of an instrument like the Nexsa has to be done through a EU tender process. As a somewhat unexpected result of this process, we were offered the Nexsa at a very favorable price. We were therefore able to squeeze <span title="The only analytical option (that means excluded chillers, factory training courses, UPS etc) not chosen is a vacuum transfer module " > ''all'' </span> but one of the available options into the budget. That is, of course, very nice indeed, but it also means that we will have to investigate the applications of the various techniques as there is no applications waiting for a specific technique to become available. | The acquisition of an instrument like the Nexsa has to be done through a EU tender process. As a somewhat unexpected result of this process, we were offered the Nexsa at a very favorable price. We were therefore able to squeeze <span title="The only analytical option (that means excluded chillers, factory training courses, UPS etc) not chosen is a vacuum transfer module " > ''all'' </span> but one of the available options into the budget. That is, of course, very nice indeed, but it also means that we will have to investigate the applications of the various techniques as there is no applications waiting for a specific technique to become available. | ||
| Line 8: | Line 10: | ||
*'''Web of Science''': Click here to access the article in the Web of Science database (log on to WoS via DTU Inside in advance, click [http://www.webofknowledge.com.proxy.findit.dtu.dk/wos '''this link''' ] ). This will enable you to browse the cited references and citations of the article. | *'''Web of Science''': Click here to access the article in the Web of Science database (log on to WoS via DTU Inside in advance, click [http://www.webofknowledge.com.proxy.findit.dtu.dk/wos '''this link''' ] ). This will enable you to browse the cited references and citations of the article. | ||
*'''Abstract''': Hover the mouse over the text to show the abstract of the article. | *'''Abstract''': Hover the mouse over the text to show the abstract of the article. | ||
{{Template:Nexsa-tableheader}} | {{Template:Nexsa-tableheader}} | ||
| | {{Template:Nexsa-addpubrow | ||
|- | |LMdocID=5385 | ||
| | |LMdocTitle=Multitechnique Surface Characterization of Organic LED Material | ||
| | |LMdocType=Application note | ||
| | |LMdocAuthor=P Mack | ||
| | |docLink=https://assets.thermofisher.com/TFS-Assets/MSD/Application-Notes/AN52109_E_Organic_LED_0411M_H_1.pdf | ||
| | |XPSused=x |UPSused=x |ISSused= |REELSused=x |Ramanused= | ||
| | |AdditionalOption= | ||
| | |Sample=Organic LED's | ||
|Abstract=Organic LED material was characterized using X-ray photoelectron spectroscopy (XPS), reflected electron energy loss spectroscopy (REELS) and ultraviolet photoelectron Organic LED material was characterized using X-ray photoelectron spectroscopy (XPS), reflected electron energy loss spectroscopy (REELS) and ultraviolet photoelectron spectroscopy (UPS). XPS was used to analyze the surface composition of the material and by combining the information from REELS and UPS a full energy level diagram of the material was created using a single instrument. | |||
| [[media:AN52476-confirming-layer-structure-organic-fet-device.pdf | | }} | ||
{{Template:Nexsa-addpubrow | |||
|LMdocID=5384 | |||
|LMdocTitle=Advantages of coincident XPS-Raman in the analysis of mineral oxides species | |||
|LMdocType=Application note | |||
|LMdocAuthor= Thermofisher Scientific | |||
|docLink=https://assets.thermofisher.com/TFS-Assets/MSD/Application-Notes/advantages-coincident-xps-raman-mineral-oxides-species-AN52994.pdf | |||
|XPSused=x |UPSused= |ISSused= |REELSused= |Ramanused=x | |||
|AdditionalOption= | |||
|Sample=TiO<sub>2</sub>, CaCO<sub>3</sub> | |||
|Abstract=X-ray photoelectron spectroscopy (XPS) and Raman spectroscopy are two popular analytical techniques due to their flexibility, ease of use, and the wealth of information they provide. Until recently analysis of a material with both of these techniques required the use of two different instruments, however the development of coincident XPSRaman allows for straightforward and quick utilisation of both techniques opening up new exciting materials characterisation opportunities. | |||
}} | |||
{{Template:Nexsa-addpubrow | |||
|LMdocID=5386 | |||
|LMdocTitle=Spectroscopic analysis of solid oxide fuel cell material with XPS | |||
|LMdocType=Application note | |||
|LMdocAuthor=P Mack | |||
|docLink=https://assets.thermofisher.com/TFS-Assets/MSD/Application-Notes/AN52110-spectroscopic-analysis-solid-oxide-fuel-cell-material-xps.pdf | |||
|XPSused=x |UPSused= |ISSused= |REELSused= |Ramanused= | |||
|AdditionalOption= | |||
|Sample= | |||
|Abstract= | |||
}} | |||
{{Template:Nexsa-addpubrow | |||
|LMdocID= | |||
|LMdocTitle=Rapid XPS image acquisition using SnapMap | |||
|LMdocType=Application note | |||
|LMdocAuthor=R Simpson | |||
|docLink=https://assets.thermofisher.com/TFS-Assets/MSD/Application-Notes/AN52330-rapid-xps-image-acquisition-using-snapmap.pdf | |||
|XPSused= |UPSused= |ISSused= |REELSused= |Ramanused= | |||
|AdditionalOption=SnapMap | |||
|Sample= | |||
|Abstract= | |||
}} | |||
{{Template:Nexsa-addpubrow | |||
|LMdocID=5388 | |||
|LMdocTitle=Composition, coverage and band gap analysis of ALD-grown ultra thin films | |||
|LMdocType=Application note | |||
|LMdocAuthor=P Mack | |||
|docLink=https://assets.thermofisher.com/TFS-Assets/MSD/Application-Notes/AN52344-composition-coverage-band-gap-aanalysis-ald-grown-ultra-thin-films.pdf | |||
|XPSused= |UPSused= |ISSused= |REELSused= |Ramanused= | |||
|AdditionalOption=Band gap | |||
|Sample=Gate dielectrics, HfO<sub>2</sub>, SiO<sub>2</sub> | |||
|Abstract= | |||
}} | |||
{{Template:Nexsa-addpubrow | |||
|LMdocID=5389 | |||
|LMdocTitle=Confirming the layer structure of an organic FET device | |||
|LMdocType=Application note | |||
|LMdocAuthor=P Mack | |||
|docLink=https://www.thermofisher.com/document-connect/document-connect.html?url=https://assets.thermofisher.com/TFS-Assets%2FMSD%2FApplication-Notes%2FAN52476-confirming-layer-structure-organic-fet-device.pdf | |||
|XPSused= |UPSused= |ISSused= |REELSused= |Ramanused= | |||
|AdditionalOption=MAGCIS | |||
|Sample=Organic FET's | |||
|Abstract= | |||
}} | |||
| [[media:AN52476-confirming-layer-structure-organic-fet-device.pdf | ]]|||| ||||X||||||||||||,|| | |||
|- | |- | ||
{{Template:Nexsa-addpubrow | {{Template:Nexsa-addpubrow | ||
Latest revision as of 11:38, 21 October 2025
Overview of the processing options on the XPS Nexsa
The acquisition of an instrument like the Nexsa has to be done through a EU tender process. As a somewhat unexpected result of this process, we were offered the Nexsa at a very favorable price. We were therefore able to squeeze all but one of the available options into the budget. That is, of course, very nice indeed, but it also means that we will have to investigate the applications of the various techniques as there is no applications waiting for a specific technique to become available.
We have therefore compiled the table below that contains articles and application notes in which several of the available techniques are used
The columns contain the following information (excluded are the columns where the content is evident):
- Title: Click on the title to access a pdf version of the article/application note.
- Web of Science: Click here to access the article in the Web of Science database (log on to WoS via DTU Inside in advance, click this link ). This will enable you to browse the cited references and citations of the article.
- Abstract: Hover the mouse over the text to show the abstract of the article.
Please don't hesitate to contact us if you find a relevant article to include in the table. Or if any of the articles listed is not suitable.