The Cleaver: LatticeAxe a scriber designed for cleaving/scribing wafers into smaller pieces without leaving any particles on the sample. It works by making a small mark in the side of the sample that is then used as a start point for the cleaving.
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.'''


The equipment is placed in the left drawer underneath fumehood 5: Special purposes. When operated the the Cleaver: lattice axe should always be placed inside Fume hood 5.
== The Cleaver: LatticeAxe ==
 
The Cleaver: LatticeAxe is designed for cleaving wafers into smaller pieces without leaving any particles on the sample. It works by making a small mark in the side of the sample that is then used as a start point for the cleaving.
 
The equipment is placed in the left drawer underneath fume hood 5: Special purposes. When operated the the Cleaver: lattice axe should always be placed inside Fume hood 5.


[[File:LatticeAxe placer prøve.JPG|400px]]
[[File:LatticeAxe placer prøve.JPG|400px]]
Line 18: Line 22:
The LatticeAxe can cleave samples from 100mm down to 10mm. In some cases it can even be used on larger samples please contact wetchemistry group for more information
The LatticeAxe can cleave samples from 100mm down to 10mm. In some cases it can even be used on larger samples please contact wetchemistry group for more information


DTU-Nanolab has 3 different types of Cleavers see the Labadviser pages for the '''[http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/FlexScribe FlexScribe]''' and the '''[http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/FlipScribe Flipscribe]''' for more information.
DTU-Nanolab has 3 different types of Cleavers see the Labadviser pages for the '''[http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/FlexScribe FlexScribe]''' and the '''[http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/FlipScribe FlipScribe]''' for more information.