Jump to content

Specific Process Knowledge/Characterization/SEM LEO: Difference between revisions

Jmli (talk | contribs)
Mmat (talk | contribs)
 
(5 intermediate revisions by 2 users not shown)
Line 1: Line 1:
{{cc-nanolab}}


'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/SEM_LEO0 click here]'''
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/SEM_LEO0 click here]'''
<br>
<br>
'''<p style="color:red;">The SEM LEO  has been decomissioned and relocated to DTU Mechanics in 2020.</p>'''


 
=SEM LEO=
=The SEM LEO has been decommissioned and relocated to DTU Mechanics=
 
[[image:IMG_3290.jpg|400x400px|right|thumb|The SEM LEO located in cleanroom F-2]]
[[image:IMG_3290.jpg|400x400px|right|thumb|The SEM LEO located in cleanroom F-2]]


The SEM LEO was a very reliable and rugged instrument that provided high quality SEM  images of most samples and it served the users of the cleanroom for many years. Excellent images on a large variety of materials such as semiconductors, semiconductor oxides or nitrides, metals, thin films and some polymers were acquired by the thousands on the SEM.  
The SEM LEO was a very reliable and rugged instrument that provided high quality SEM  images of most samples and it served the users of the cleanroom for many years. Excellent images on a large variety of materials such as semiconductors, semiconductor oxides or nitrides, metals, thin films and some polymers were acquired by the thousands on the SEM.  


In her later years the SEM LEO was equipped with a Raith e-beam lithography system and was exclusively dedicated to the users of the Raith E-beam lithography. Decommissioned in early summer 2020, she is at DTU Mechanics.
In her later years the SEM LEO was equipped with a Raith e-beam lithography system and was exclusively dedicated to the users of the Raith E-beam lithography.
 
'''The user manual, control instruction and the user APV can still be found in LabManager:'''
 
[http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=37 SEM LEO info page in LabManager],
 
 
 
== Performance information ==
 
*[[Specific Process Knowledge/Characterization/SEM: Scanning Electron Microscopy|SEM comparison page]]
 
*[[Specific Process Knowledge/Lithography/EBeamLithography/RaithElphy|Raith Elphy e-beam lithography system]]


===Typical current values for EBL===
===Typical current values for EBL===