Specific Process Knowledge/Etch/Etching of Bulk Glass: Difference between revisions
Appearance
| (2 intermediate revisions by 2 users not shown) | |||
| Line 1: | Line 1: | ||
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.''' | |||
'''All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.''' | |||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Etching_of_Bulk_Glass click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Etching_of_Bulk_Glass click here]''' | ||
<!-- Replace "http://labadviser.nanolab.dtu.dk/..." with the link to the Labadviser page--> | <!-- Replace "http://labadviser.nanolab.dtu.dk/..." with the link to the Labadviser page--> | ||
| Line 4: | Line 8: | ||
== Comparing methods for etching bulk glass at DTU Nanolab == | == Comparing methods for etching bulk glass at DTU Nanolab == | ||
Etching of glass can be done either wet or dry. Wet etching is done with HF. Dry etching can be done either with [[Specific Process Knowledge/Etch/AOE (Advanced Oxide Etch)|AOE]] using fluorine chemistry (only fused silica) or with [[Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE]] by sputtering with Ar ions and/or using fluorine chemistry. | Etching of glass can be done either wet or dry. Wet etching is done with HF. Dry etching can be done either with [[Specific Process Knowledge/Etch/AOE (Advanced Oxide Etch)|AOE]], ASE or Pegasus 4 using fluorine chemistry (only fused silica) or with [[Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE]] by sputtering with Ar ions and/or using fluorine chemistry. | ||
At DTU Nanolab, we have two types of bulk glass substrates: Borosilicate glass (Borofloat 33 (like pyrex)) and fused silica glass which in cleanliness is similar to quartz. Both types are etched wet in a special set-up placed in a fumehood using a concentrated HF-solution (isotropic etch). | At DTU Nanolab, we have two types of bulk glass substrates: Borosilicate glass (Borofloat 33 (like pyrex)) and fused silica glass which in cleanliness is similar to quartz. Both types are etched wet in a special set-up placed in a fumehood using a concentrated HF-solution (isotropic etch). | ||