Jump to content

Specific Process Knowledge/Etch/Titanium Oxide/ICP metal: Difference between revisions

From LabAdviser
Bghe (talk | contribs)
No edit summary
Bghe (talk | contribs)
m Reverted edit by Prakus (talk) to last revision by Bghe
Tag: Rollback
 
(6 intermediate revisions by 3 users not shown)
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Titanium_Oxide/ICP_metal click here]'''  
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Titanium_Oxide/ICP_metal click here]'''  
<!--Checked for updates on 11/2-2019 - ok/jmli -->




===Etching of TiO2 using ICP metal has been tested Evgeniy Shkondin, DTU Nanolab===


===Etching of TiO2 using ICP metal has been tested Evgeniy Shkondin @danchip===
Recipe used: Ti etch <br>
 
Recipe used: Ti etch
[[image:TiO2_etch_Evgeniy2.jpg|400px]]
[[image:TiO2_etch_Evgeniy2.jpg|400px]]

Latest revision as of 15:16, 4 September 2025

Feedback to this page: click here


Etching of TiO2 using ICP metal has been tested Evgeniy Shkondin, DTU Nanolab

Recipe used: Ti etch