Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-2/TemperatureSettings: Difference between revisions
Appearance
No edit summary |
|||
| (2 intermediate revisions by the same user not shown) | |||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/DRIE-Pegasus/Pegasus-2 click here]''' | |||
<!--Checked for updates on 28/6-2023 - ok/jmli --> | |||
<!--Checked for updates on 4/9-2025 - ok/jmli --> | |||
{{contentbydryetch}} | |||
==Correct settings for temperatures on Pegasus 2 == | ==Correct settings for temperatures on Pegasus 2 == | ||
The Platen chiller temperature is enabled and the setpoint is 20 degrees. This setting could be applied to all the heaters, however, the best way by far is to run the processes without enabling | The Platen chiller temperature is enabled and the setpoint is 20 degrees as seen in the image below. This setting could be applied to all the heaters, however, the best way by far is to run the processes without enabling the heaters as seen for the other heaters. | ||
[[file:Peg2tempsettings.jpg | 400px | frameless]] | [[file:Peg2tempsettings.jpg | 400px | frameless]] | ||
Latest revision as of 12:00, 4 September 2025
Feedback to this page: click here
Unless otherwise stated, the content of this page was created by the dry etch group at DTU Nanolab
Correct settings for temperatures on Pegasus 2
The Platen chiller temperature is enabled and the setpoint is 20 degrees as seen in the image below. This setting could be applied to all the heaters, however, the best way by far is to run the processes without enabling the heaters as seen for the other heaters.