Specific Process Knowledge/Etch/DRIE-Pegasus/processA/PrA-2: Difference between revisions
Appearance
Created page with " {| border="2" cellpadding="0" cellspacing="0" style="text-align:center;" |+ '''Process runs''' |- ! rowspan="2" width="40"| Date ! colspan="2" width="120"| Substrate Informa..." |
No edit summary |
||
| (5 intermediate revisions by the same user not shown) | |||
| Line 1: | Line 1: | ||
'''Feedback to this page''': | |||
'''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/DRIE-Pegasus/processA/PrA-2 click here]''' | |||
<!--Checked for updates on 30/7-2018 - ok/jmli --> | |||
<!--Checked for updates on 5/10-2020 - ok/jmli --> | |||
<!--Checked for updates on 28/6-2023 - ok/jmli --> | |||
{{contentbydryetch}} | |||
<!--Checked for updates on 4/9-2025 - ok/jmli --> | |||
{| border="2" cellpadding="0" cellspacing="0" style="text-align:center;" | {| border="2" cellpadding="0" cellspacing="0" style="text-align:center;" | ||
| Line 7: | Line 13: | ||
! colspan="2" width="120"| Substrate Information | ! colspan="2" width="120"| Substrate Information | ||
! colspan="3" | Process Information | ! colspan="3" | Process Information | ||
! rowspan="2 | ! rowspan="2" |SEM Images | ||
|- | |- | ||
! width="30" | Wafer info | ! width="30" | Wafer info | ||
| Line 22: | Line 28: | ||
| C03991.03 | | C03991.03 | ||
| | | | ||
[[file:C03991.03 103.jpg|150px|frameless ]] | |||
[[file:C03991.03 104.jpg|150px|frameless ]] | |||
[[file:C03991.03 105.jpg|150px|frameless ]] | |||
[[file:C03991.03 106.jpg|150px|frameless ]] | |||
[[file:C03991.03 107.jpg|150px|frameless ]] | [[file:C03991.03 107.jpg|150px|frameless ]] | ||
[[file:C03991.03 108.jpg|150px|frameless ]] | [[file:C03991.03 108.jpg|150px|frameless ]] | ||
| Line 36: | Line 45: | ||
[[file:C03991.03 118.jpg|150px|frameless ]] | [[file:C03991.03 118.jpg|150px|frameless ]] | ||
[[file:C03991.03 119.jpg|150px|frameless ]] | [[file:C03991.03 119.jpg|150px|frameless ]] | ||
|- | |- | ||
| 2/5-2016 | | 2/5-2016 | ||
| Line 49: | Line 53: | ||
| C03991.06 | | C03991.06 | ||
| | | | ||
[[file:C03991.06 152.jpg|150px|frameless ]] | |||
[[file:C03991.06 153.jpg|150px|frameless ]] | |||
[[file:C03991.06 154.jpg|150px|frameless ]] | [[file:C03991.06 154.jpg|150px|frameless ]] | ||
[[file:C03991.06 155.jpg|150px|frameless ]] | [[file:C03991.06 155.jpg|150px|frameless ]] | ||
| Line 65: | Line 71: | ||
[[file:C03991.06 168.jpg|150px|frameless ]] | [[file:C03991.06 168.jpg|150px|frameless ]] | ||
[[file:C03991.06 169.jpg|150px|frameless ]] | [[file:C03991.06 169.jpg|150px|frameless ]] | ||
|- | |- | ||
| 3/6-2016 | | 3/6-2016 | ||
| Line 76: | Line 79: | ||
| C04047.03 | | C04047.03 | ||
| | | | ||
[[file:C04047.03 109.jpg|150px|frameless ]] | |||
[[file:C04047.03 108.jpg|150px|frameless ]] | |||
[[file:C04047.03 107.jpg|150px|frameless ]] | |||
[[file:C04047.03 106.jpg|150px|frameless ]] | |||
[[file:C04047.03 105.jpg|150px|frameless ]] | |||
[[file:C04047.03 104.jpg|150px|frameless ]] | |||
[[file:C04047.03 103.jpg|150px|frameless ]] | |||
[[file:C04047.03 102.jpg|150px|frameless ]] | |||
[[file:C04047.03 101.jpg|150px|frameless ]] | |||
[[file:C04047.03 100.jpg|150px|frameless ]] | |||
[[file:C04047.03 099.jpg|150px|frameless ]] | [[file:C04047.03 099.jpg|150px|frameless ]] | ||
[[file:C04047.03 | [[file:C04047.03 098.jpg|150px|frameless ]] | ||
[[file:C04047.03 097.jpg|150px|frameless ]] | [[file:C04047.03 097.jpg|150px|frameless ]] | ||
|- | |- | ||
| Line 98: | Line 101: | ||
| C04047.06 | | C04047.06 | ||
| | | | ||
[[file:C04047.06 153.jpg|150px|frameless ]] | |||
[[file:C04047.06 152.jpg|150px|frameless ]] | |||
[[file:C04047.06 151.jpg|150px|frameless ]] | |||
[[file:C04047.06 150.jpg|150px|frameless ]] | |||
[[file:C04047.06 149.jpg|150px|frameless ]] | |||
[[file:C04047.06 148.jpg|150px|frameless ]] | |||
[[file:C04047.06 147.jpg|150px|frameless ]] | |||
[[file:C04047.06 146.jpg|150px|frameless ]] | |||
[[file:C04047.06 145.jpg|150px|frameless ]] | [[file:C04047.06 145.jpg|150px|frameless ]] | ||
[[file:C04047.06 | [[file:C04047.06 144.jpg|150px|frameless ]] | ||
[[file:C04047.06 | [[file:C04047.06 143.jpg|150px|frameless ]] | ||
[[file:C04047.06 | [[file:C04047.06 142.jpg|150px|frameless ]] | ||
[[file:C04047.06 | [[file:C04047.06 141.jpg|150px|frameless ]] | ||
[[file:C04047.06 150.jpg|150px|frameless ]] | [[file:C04047.06 150.jpg|150px|frameless ]] | ||
[[file:C04047.06 139.jpg|150px|frameless ]] | [[file:C04047.06 139.jpg|150px|frameless ]] | ||
|- | |- | ||
|} | |} | ||
Latest revision as of 10:41, 4 September 2025
Feedback to this page: click here Unless otherwise stated, the content of this page was created by the dry etch group at DTU Nanolab
| Date | Substrate Information | Process Information | SEM Images | |||
|---|---|---|---|---|---|---|
| Wafer info | Exposed area | Conditioning | Recipe | Wafer ID | ||
| 2/5-2016 | 4" Travka20 Wafer | 20 % Si | 3 minute TDESC clean | PrA-2, 80 cycles or 14:40 minutes | C03991.03 | |
| 2/5-2016 | 4" Travka20 Wafer | 20 % Si | 3 minute TDESC clean | PrA-2, 80 cycles or 14:40 minutes | C03991.06 | |
| 3/6-2016 | 4" Travka20 Wafer | 20 % Si | 3 minute TDESC clean | PrA-2, 80 cycles or 14:40 minutes | C04047.03 | |
| 3/6-2016 | 4" Travka20 Wafer | 20 % Si | 3 minute TDESC clean | PrA-2, 80 cycles or 14:40 minutes | C04047.06 | |