Specific Process Knowledge/Characterization/XPS/XPS Depth profiling: Difference between revisions
Appearance
No edit summary |
|||
| (11 intermediate revisions by the same user not shown) | |||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@ | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Characterization/XPS/XPS_Depth_profiling click here]''' | ||
<!--Checked for updates on 24/8-2021. ok/ jmli--> | |||
<!-- Page reviewed 8/5-2023 jmli --> | |||
{{Author-jmli1}} | |||
<!--Checked for updates on 4/9-2025 - ok/jmli --> | |||
=Depth profiling= | =Depth profiling= | ||
| Line 15: | Line 19: | ||
* Polysilicon | * Polysilicon | ||
[[File:profile sandwich 3.PNG|700px]] | [[File:profile sandwich 3.PNG|700px|{{photo1}}]] | ||
In the spectra required to make such a depth profile, one can distinguish the various chemical environments of silicon depending on whether it is bonded to: | |||
* Silicon as in the bulk (oxidation state 0). | |||
* Oxygen, either fully oxidized (oxidation state IV) in SiO<sub>2</sub> or in intermediate states with a mixture of silicon and oxygen bonds (oxidation state I, II and III) | |||
* Nitrogen, also fully oxidized (oxidation state IV) | |||
and plot their atomic percentages along with the percentages of oxygen and nitrogen. | |||