Jump to content

Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange/SOI/SOI: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
No edit summary
Jmli (talk | contribs)
No edit summary
 
(One intermediate revision by the same user not shown)
Line 1: Line 1:
  <!-- Ok, jmli 20170627 -->
  <!-- Ok, jmli 20170627 -->
<!-- Page reviewed 9/8-2022 jmli -->
<!-- Page reviewed 9/8-2022 jmli -->
 
{{Author-jmli1}}
 
<!--Checked for updates on 4/9-2025 - ok/jmli -->
 


{| border="2" cellpadding="0" cellspacing="0" style="text-align:center;"
{| border="2" cellpadding="0" cellspacing="0" style="text-align:center;"

Latest revision as of 10:32, 4 September 2025

Unless otherwise stated, all content on this page was created by Jonas Michael-Lindhard, DTU Nanolab

Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
15/12-2014 4" Wafer with travka65 mask AZ standard Si / 65 % Pegasus/jmli 10 minute TDESC clean nanolab/jml/showerhead/SOI/SOI, 96 cyc or 8:00 mins S004745 New showerhead