==Barc etch with O2==
==Barc etch with O2==
{{CC-bghe2}}''June 2020''
{{CC-bghe2}}, ''June 2020''
===Sample===
===Sample===
*6" Si
*6" Si
* 2µm SiO2 from C1
* 2 µm SiO2 from C1
*90nm barc
*90 nm barc
*907 nm UVN 2030-0,5
*907 nm UVN 2030-0,5
*Reticle: Pegreticle
*Reticle: Pegreticle

Latest revision as of 09:31, 4 September 2025

Barc etch with O2

Unless otherwise stated, all content in this section was done by Berit Herstrøm, DTU Nanolab, June 2020

Sample

  • 6" Si
  • 2 µm SiO2 from C1
  • 90 nm barc
  • 907 nm UVN 2030-0,5
  • Reticle: Pegreticle
  • Dose: 200 J/m2

Pegasus 4 settings

  • Recipe: Barc O2
  • With 30 mm spacers

SEM images after barc etching