''By Berit Herstrøm, DTU Nanolab June 2020''
{{CC-bghe2}}, ''June 2020''
===Sample===
===Sample===
*6" Si
*6" Si
* 2µm SiO2 from C1
* 2 µm SiO2 from C1
*90nm barc
*90 nm barc
*907 nm UVN 2030-0,5
*907 nm UVN 2030-0,5
*Reticle: Pegreticle
*Reticle: Pegreticle