== Silicon etching on the ICP Metal Etcher ==
== Silicon etching on the ICP Metal Etcher ==

Latest revision as of 10:28, 4 September 2025

Feedback to this page: click here

Silicon etching on the ICP Metal Etcher

Unless otherwise stated, all content on this page was created by Jonas Michael-Lindhard, DTU Nanolab

In the primary silicon etcher at Nanolab, the DRIE-Pegasus, silicon is etched using a fluorine based plasma (with SF6 as etch gas). Silicon is also etched by chlorine and bromine.