Jump to content

Specific Process Knowledge/Etch/ICP Metal Etcher/silicon: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
No edit summary
Jmli (talk | contribs)
No edit summary
 
(3 intermediate revisions by the same user not shown)
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/ICP_Metal_Etcher/silicon click here]'''  
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/ICP_Metal_Etcher/silicon click here]'''  
<!--Checked for updates on 30/7-2018 - ok/jmli -->
<!--Checked for updates on 30/7-2018 - ok/jmli -->
<!--Page reviewed by jmli 9/8-2022  -->
<!--Checked for updates on 4/9-2025 - ok/jmli -->
== Silicon etching on the ICP Metal Etcher ==
== Silicon etching on the ICP Metal Etcher ==
<!--Page reviewed by jmli 2/2-2023  -->
{{Template:Author-jmli1}}


In the primary silicon etcher at Danchip, the [[Specific Process Knowledge/Etch/DRIE-Pegasus|DRIE-Pegasus]], silicon is etched using a fluorine based plasma (with SF<sub>6</sub> as etch gas). Silicon is also etched by chlorine and bromine.
In the primary silicon etcher at Nanolab, the [[Specific Process Knowledge/Etch/DRIE-Pegasus|DRIE-Pegasus]], silicon is etched using a fluorine based plasma (with SF<sub>6</sub> as etch gas). Silicon is also etched by chlorine and bromine.


*[[Specific Process Knowledge/Etch/ICP Metal Etcher/silicon/nano|Chlorine/Bromine etch of nanostructures in silicon]]
*[[Specific Process Knowledge/Etch/ICP Metal Etcher/silicon/nano|Chlorine/Bromine etch of nanostructures in silicon]]


*[[Specific Process Knowledge/Etch/ICP Metal Etcher/silicon/isotropic| Isotropic etching in silicon]]
*[[Specific Process Knowledge/Etch/ICP Metal Etcher/silicon/isotropic| Isotropic etching in silicon]]

Latest revision as of 10:28, 4 September 2025

Feedback to this page: click here

Silicon etching on the ICP Metal Etcher

Unless otherwise stated, all content on this page was created by Jonas Michael-Lindhard, DTU Nanolab

In the primary silicon etcher at Nanolab, the DRIE-Pegasus, silicon is etched using a fluorine based plasma (with SF6 as etch gas). Silicon is also etched by chlorine and bromine.