Specific Process Knowledge/Etch/ICP Metal Etcher/Aluminium: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| (5 intermediate revisions by the same user not shown) | |||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@ | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/ICP_Metal_Etcher/Aluminium click here]''' | ||
<!--Checked for updates on 30/7-2018 - ok/jmli --> | <!--Checked for updates on 30/7-2018 - ok/jmli --> | ||
<!--Page reviewed by jmli 9/8-2022 --> | |||
<!--Checked for updates on 4/9-2025 - ok/jmli --> | |||
=== Aluminium etch === | === Aluminium etch === | ||
{{Template:Author-jmli1}} | |||
<!--Checked for updates on 2/02-2023 - ok/jmli --> | |||
The aluminium etch has two steps: | The aluminium etch has two steps: | ||
| Line 65: | Line 69: | ||
{| border="2" cellpadding="2" cellspacing="1" style="text-align:center;" | {| border="2" cellpadding="2" cellspacing="1" style="text-align:center;" | ||
|+ '''Al etch''' ''made by Chantal Silvetre@ | |+ '''Al etch''' ''made by Chantal Silvetre@nanolab October 2014'' | ||
|- | |- | ||
! rowspan="2" | Parameter | ! rowspan="2" | Parameter | ||
| Line 113: | Line 117: | ||
|~282 nm/min (depending on features size and etch load) | |~282 nm/min (depending on features size and etch load) | ||
|} | |} | ||