Here is a table with 2 different imprint resists we have recently used in the cleanroom, with links to a purchase manufactor, technical reports about resist properties and a current process flow, tested in our cleanroom.  
Here is a table with 2 different imprint resists we have recently used in the cleanroom, with links to a purchase manufactor, technical reports about resist properties and a current process flow, tested in our cleanroom.  


{|border="1" cellspacing="1" cellpadding="3" style="text-align:left;" width="95%"
{|border="1" cellspacing="1" cellpadding="10" style="text-align:left;"  
|-
|-


Line 35: Line 35:
|'''mr-I 7030R'''
|'''mr-I 7030R'''
| [http://www.microresist.de/en/products/nanoimprint-resists/thermal-nanoimprint-lithography/mr-i-7000r-series micro resist technology]
| [http://www.microresist.de/en/products/nanoimprint-resists/thermal-nanoimprint-lithography/mr-i-7000r-series micro resist technology]
|We purchase only mr-I 7030R, for use it please contact [mailto:Lithography@nanolab.dtu.dk Lithography].
|We purchase only mr-I 7030R, to use it please contact [mailto:Lithography@nanolab.dtu.dk Lithography].
|[[media:PI_mr_I_7000R_8000R_2017.pdf|mr-I 7030R.pdf]]
|[[media:PI_mr_I_7000R_8000R_2017.pdf|mr-I 7030R.pdf]]
|mr-T 1050
|mr-T 1050

Latest revision as of 13:36, 25 August 2025

Imprint Resist Overview

Here is a table with 2 different imprint resists we have recently used in the cleanroom, with links to a purchase manufactor, technical reports about resist properties and a current process flow, tested in our cleanroom.

Resist Manufacturer Comments Technical reports Thinner Spinner Rinse Process flows (in docx-format)
Topas micro resist technology Users may purchase own resist. Topas.pdf LabSpin03 or LabSpin03 IPA
mr-I 7030R micro resist technology We purchase only mr-I 7030R, to use it please contact Lithography. mr-I 7030R.pdf mr-T 1050 LabSpin03 or LabSpin03 Acetone Preparation substrate with mr-I 7030R: Preparation substrate‎ with imprint layer