Specific Process Knowledge/Lithography/Resist/DUVresist: Difference between revisions
Appearance
Created page with "'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Lithography/Resist/DUVresist click here]''' ==DUV resist== The spinning process will be performed by the customer together with the Photolith group of Nanolab. In case you would like to do DUV lithography please contact Lithography team, who will consult you and run your wafers together with you. In..." |
mNo edit summary |
||
| (7 intermediate revisions by one other user not shown) | |||
| Line 1: | Line 1: | ||
===DUV resist overview=== | |||
The spinning process will be performed by the customer together with the Photolith group of Nanolab. In case you would like to do DUV lithography, please contact Lithography team, who will consult you and run your wafers together with you. | |||
'''Bottom Anti Reflection Coating (BARC):''' | |||
*Manufacturers website: [http://www.brewerscience.com/products/arc/dry-etch-arc-coatings/248nm-products/duv42s DUV 42S-6] | |||
*Datasheet: [https://labmanager.dtu.dk/view_binary.php?class=MiscDocument&id=4&name=Datasheet+DUV42S.pdf DUV42S-6] - '''requires login''' | |||
* | |||
'''Positive DUV resist for spin coating in 600-300nm thickness range:''' | |||
* | *Manufacturers website: [https://www.jsrmicro.be/semiconductor/lithography/jsr-krf-photoresists KrF M230Y] | ||
*Datasheet: [https://labmanager.dtu.dk/view_binary.php?class=MiscDocument&id=4&name=datasheet+M230Y.pdf KrF M230Y] - '''requires login''' | |||
'''Positive DUV resist for spin coating in 1600-800nm thickness range:''' | |||
*Manufacturers website: [https://www.jsrmicro.be/semiconductor/lithography/jsr-krf-photoresists KrF M35G] | |||
*Datasheet: [https://labmanager.dtu.dk/view_binary.php?class=MiscDocument&id=4&name=datasheet+M35G.pdf KrF M35G] - '''requires login''' | |||
'''Negative DUV resist for spin coating in 1400-800nm or diluted with EC Solvent in 1:1 in 400-200nm thickness range:''' | |||
*Manufacturers website: [https://www.microresist.de/en/produkt/uvn-2300-series/ UVN2300-0.8] | |||
*Datasheet: [https://labmanager.dtu.dk/view_binary.php?class=MiscDocument&id=4&name=datasheet+UVN2300.pdf UVN2300-0.8] - '''requires login''' | |||
Latest revision as of 13:31, 25 August 2025
DUV resist overview
The spinning process will be performed by the customer together with the Photolith group of Nanolab. In case you would like to do DUV lithography, please contact Lithography team, who will consult you and run your wafers together with you.
Bottom Anti Reflection Coating (BARC):
Positive DUV resist for spin coating in 600-300nm thickness range:
Positive DUV resist for spin coating in 1600-800nm thickness range:
Negative DUV resist for spin coating in 1400-800nm or diluted with EC Solvent in 1:1 in 400-200nm thickness range:
- Manufacturers website: UVN2300-0.8
- Datasheet: UVN2300-0.8 - requires login