==Sputtering of Nickel Vanadium==
==Sputtering of Nickel Vanadium==


Nickel Vanadium may be sputter deposited in the Sputter-system (Lesker) and the Sputter-system Metal-Oxide. The following pages show both process parameters and data on surface roughness of the deposited films:
Nickel Vanadium may be sputter deposited in the Sputter-system (Lesker) and the Sputter-system Metal-Oxide (PC1). The following pages show both process parameters and data on surface roughness of the deposited films:


* [[/Sputtering of NiV in Lesker|Sputtering of NiV in Lesker]]
* [[/Sputtering of NiV in Lesker|Sputtering of NiV in Sputter-System (Lesker)]]
* [[/Sputtering of NiV in Sputter-System Metal-Oxide (PC1)|Sputtering of NiV in Sputter-System Metal-Oxide (PC1)]]
* [[/Sputtering of NiV in Sputter-System Metal-Oxide (PC1)|Sputtering of NiV in Sputter-System Metal-Oxide (PC1)]]
* [[/Sputtering of NiV in Wordentec|Sputtering of NiV in Wordentec]] (tool now decommissioned, but results may be of general interest)
* [[/Sputtering of NiV in Wordentec|Sputtering of NiV in Wordentec]] (tool now decommissioned, but results are of general interest)




Line 108: Line 108:
*Substrate rotation
*Substrate rotation
*Substrate RF Bias (optional)
*Substrate RF Bias (optional)
*Substrate heating to 600 C


|-
|-

Latest revision as of 11:11, 18 July 2025

Feedback to this page: click here

Sputtering of Nickel Vanadium

Nickel Vanadium may be sputter deposited in the Sputter-system (Lesker) and the Sputter-system Metal-Oxide (PC1). The following pages show both process parameters and data on surface roughness of the deposited films:


In the chart below you can compare the available sputter systems:

Sputter deposition (Sputter-System Lesker) Sputter deposition (Sputter-system Metal-Oxide (PC1) and Sputter-system Metal-Nitride (PC3))
General description Sputter deposition of NiV Sputter deposition of NiV
Pre-clean none RF Ar clean
Layer thickness About 10Å to 5000Å About 10Å to 5000Å
Deposition rate Depending on process parameters(normally less than 1 Å/s). Depending on process parameters(normally less than 1 Å/s).
Batch size
  • Pieces or
  • 1x4" wafer or
  • 1x6" wafer
  • Up to 10x4" or 6" wafers
  • Many smaller pieces
Allowed substrates
  • Silicon wafers
  • Quartz wafers
  • Pyrex wafers(No substrate heating)
  • Almost any that do not outgas.
Allowed materials
  • Silicon
  • Silicon oxide
  • Silicon nitride
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
  • Carbon
  • Almost any that do not outgas.


Target size 2 inch sputter target 3 inch sputter target

(or in special cases 4 inch)

Comment
  • Sputter target with NiV composition: Ni/V 93/7%
  • Substrate rotation
  • Sputter target with NiV composition: Ni/V 93/7%
  • Substrate rotation
  • Substrate RF Bias (optional)
  • Substrate heating to 600 C