==Sputtering of Molybdenum== | ==Sputtering of Molybdenum== | ||
Molybdenum may be sputter deposited in either the single-chamber sputter-system ("Sputter System Lesker") or the cluster-based sputter system ("Sputter-System Metal-Oxide(PC1)" and "Sputter-System Metal-Nitride(PC3)"). See more in link here and the chart below. | Molybdenum may be sputter deposited in either the single-chamber sputter-system ("Sputter System Lesker") or the cluster-based sputter system ("[[Specific Process Knowledge/Thin film deposition/Cluster-based multi-chamber high vacuum sputtering deposition system|Sputter-System Metal-Oxide(PC1)]]" and "[[Specific Process Knowledge/Thin film deposition/Cluster-based multi-chamber high vacuum sputtering deposition system|Sputter-System Metal-Nitride(PC3)]]"). See more in link here and the chart below. | ||
*[[Specific Process Knowledge/Thin film deposition/Deposition of Molybdenum/Mo Sputtering in Cluster Lesker PC1|Mo Sputtering in Sputter-System Metal-Oxide(PC1)]] | *[[Specific Process Knowledge/Thin film deposition/Deposition of Molybdenum/Mo Sputtering in Cluster Lesker PC1|Mo Sputtering in Sputter-System Metal-Oxide(PC1)]] | ||
{| border="1" cellspacing="0" cellpadding="4" | {| border="1" cellspacing="0" cellpadding="4" | ||