'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_TiW click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_TiW click here]''' | ||
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i> | |||
==Sputtering of TiW== | ==Sputtering of TiW== | ||
Deposition of TiW alloy | Deposition of TiW alloy was done in the past in the [[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec]]. This tool is now decommissioned, and if necessary processes may be developed for depositing TiW in the Lesker sputter setups (contact responsible staff for this). | ||
*[[/Sputtering of TiW in Wordentec|Sputtering of TiW in Wordentec]] | *[[/Sputtering of TiW in Wordentec|Sputtering of TiW in Wordentec]] | ||
*[[Specific Process Knowledge/Thin film deposition/Deposition of TiW/Sputtering of TiW in Wordentec/Grain size and uniformity of TiW layers|Results of a study on the grain size and uniformity of TiW sputtered in the Wordentec]] | *[[Specific Process Knowledge/Thin film deposition/Deposition of TiW/Sputtering of TiW in Wordentec/Grain size and uniformity of TiW layers|Results of a study on the grain size and uniformity of TiW sputtered in the Wordentec]] | ||