'''Feedback to this page''': '''[mailto:danchipsupport@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Back-end_processing/Die_Bonder click here]''' | '''Feedback to this page''': '''[mailto:danchipsupport@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Back-end_processing/Die_Bonder click here]''' | ||
= | '''<p style="color:red;">The Polisher/Lapper has been decomissioned end of 2024.</p> | ||
== Polisher/Lapper == | |||
The Logitech PM5 Polisher/Lapper is for thinning down wafers and other substrates. | |||
==Equipment performance and process related parameters== | ==Equipment performance and process related parameters== | ||
[[File:IMG_20230228_113121.jpg|thumb|350px|PM5 lapper in Fume hood]] | |||
{| border="2" cellspacing="0" cellpadding="2" | {| border="2" cellspacing="0" cellpadding="2" | ||
!colspan="2" border="none" style="background:silver; color:black;" align="center"|Equipment | !colspan="2" border="none" style="background:silver; color:black;" align="center"|Equipment | ||
|style="background:WhiteSmoke; color:black"|<b>Polisher/Lapper</b> | |style="background:WhiteSmoke; color:black"|<b>Polisher/Lapper</b> | ||
|style="background:WhiteSmoke; color:black"|<b>Equipment 2</b> | <!-- |style="background:WhiteSmoke; color:black"|<b>Equipment 2</b> --> | ||
|- | |- | ||
!style="background:silver; color:black;" align="center" width="60"|Purpose | !style="background:silver; color:black;" align="center" width="60"|Purpose | ||
| Line 31: | Line 29: | ||
*Metals | *Metals | ||
*Glass/Quartz | *Glass/Quartz | ||
|style="background:WhiteSmoke; color:black"| | <!-- |style="background:WhiteSmoke; color:black"| | ||
*Purpose 1 | *Purpose 1 | ||
*Purpose 2 | *Purpose 2 | ||
*Purpose 3 | *Purpose 3 --> | ||
|- | |- | ||
!style="background:silver; color:black" align="center" valign="center" rowspan="2"|Performance | !style="background:silver; color:black" align="center" valign="center" rowspan="2"|Performance | ||
| Line 43: | Line 41: | ||
*Thickness homogeneity: +/- 10 µm | *Thickness homogeneity: +/- 10 µm | ||
*Roughness: +/- ? µm | *Roughness: +/- ? µm | ||
|style="background:WhiteSmoke; color:black"| | <!-- |style="background:WhiteSmoke; color:black"| | ||
*Performance range 1 | *Performance range 1 | ||
*Performance range 2 | *Performance range 2 | ||
*Performance range 3 | *Performance range 3 --> | ||
|- | |- | ||
|style="background:LightGrey; color:black"|Polishing | |style="background:LightGrey; color:black"|Polishing | ||
| Line 54: | Line 52: | ||
*Thickness homogeneity: ? µm | *Thickness homogeneity: ? µm | ||
*Roughness: +/- ? µm | *Roughness: +/- ? µm | ||
|style="background:WhiteSmoke; color:black"| | <!-- |style="background:WhiteSmoke; color:black"| | ||
*Performance range | *Performance range --> | ||
|- | |- | ||
!style="background:silver; color:black" align="center" valign="center" rowspan=" | !style="background:silver; color:black" align="center" valign="center" rowspan="4"|Process parameter range | ||
|style="background:LightGrey; color:black"|Polishing liquid | |style="background:LightGrey; color:black"|Polishing liquid | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*Al2O3 (alumina) powder: 3, 9 or 20 µm | *Al2O3 (alumina) powder: 3, 9 or 20 µm | ||
*Chemlox (for polishing) | *Chemlox (for polishing) | ||
*SF1 Polishing Fluid (for polishing e.g. SiO2) | |||
|- | |||
|style="background:LightGrey; color:black"|Polishing cloths | |||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
* | *Chemcloth Polishing Cloths (for use with SF1 liquid) | ||
|- | |- | ||
|style="background:LightGrey; color:black"|Rotation speed | |style="background:LightGrey; color:black"|Rotation speed | ||
| Line 69: | Line 70: | ||
*Thinning: 5-20 rpm | *Thinning: 5-20 rpm | ||
*Polishing: 5-80 rpm | *Polishing: 5-80 rpm | ||
|- | |- | ||
|style="background:LightGrey; color:black"|Arm sweep | |style="background:LightGrey; color:black"|Arm sweep | ||
| Line 76: | Line 75: | ||
*Thinning: stationary | *Thinning: stationary | ||
*Polishing: 12% (inner) - 80% (outer) | *Polishing: 12% (inner) - 80% (outer) | ||
|- | |- | ||
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Substrates | !style="background:silver; color:black" align="center" valign="center" rowspan="3"|Substrates | ||
| Line 83: | Line 80: | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*<nowiki>#</nowiki> small samples | *<nowiki>#</nowiki> small samples | ||
* | *one 50 mm wafer | ||
* | *one 100 mm wafer | ||
|style="background:WhiteSmoke; color:black"| | <!-- |style="background:WhiteSmoke; color:black"| | ||
*<nowiki>#</nowiki> small samples | *<nowiki>#</nowiki> small samples | ||
*<nowiki>#</nowiki> 50 mm wafers | *<nowiki>#</nowiki> 50 mm wafers | ||
*<nowiki>#</nowiki> 100 mm wafers | *<nowiki>#</nowiki> 100 mm wafers | ||
*<nowiki>#</nowiki> 150 mm wafers | *<nowiki>#</nowiki> 150 mm wafers --> | ||
|- | |- | ||
| style="background:LightGrey; color:black"|Allowed materials | | style="background:LightGrey; color:black"|Allowed materials | ||
| Line 98: | Line 95: | ||
*Metals | *Metals | ||
*Glass/Quartz | *Glass/Quartz | ||
|style="background:WhiteSmoke; color:black"| | <!-- |style="background:WhiteSmoke; color:black"| | ||
*Allowed material 1 | *Allowed material 1 | ||
*Allowed material 2 | *Allowed material 2 | ||
*Allowed material 3 | *Allowed material 3 --> | ||
|- | |- | ||
|} | |} | ||
[[File:IMG_20230228_113134.jpg|thumb|left|300px|lapping jig]] | |||
[[File:IMG_20230228_113127.jpg|thumb|1000px|mounting/measuring space]] | |||
<br clear="all" /> | <br clear="all" /> | ||
Latest revision as of 17:54, 17 June 2025
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here
The Polisher/Lapper has been decomissioned end of 2024.
Polisher/Lapper
The Logitech PM5 Polisher/Lapper is for thinning down wafers and other substrates.

| Equipment | Polisher/Lapper | |
|---|---|---|
| Purpose |
Thinning of substrates of |
|
| Performance | Thinning |
|
| Polishing |
| |
| Process parameter range | Polishing liquid |
|
| Polishing cloths |
| |
| Rotation speed |
| |
| Arm sweep |
| |
| Substrates | Batch size |
|
| Allowed materials |
| |