Specific Process Knowledge/Thin film deposition/Furnace LPCVD Nitride: Difference between revisions
Appearance
mNo edit summary |
|||
| (5 intermediate revisions by 2 users not shown) | |||
| Line 1: | Line 1: | ||
{{cc-nanolab}} | |||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Furnace_LPCVD_Nitride click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Furnace_LPCVD_Nitride click here]''' | ||
[[Category: Equipment|Thin film F]] | [[Category: Equipment|Thin film F]] | ||
[[Category: Thin Film Deposition|LPCVD nitride]] | [[Category: Thin Film Deposition|LPCVD nitride]] | ||
[[Category: Furnaces|LPCVD nitride]] | [[Category: Furnaces|LPCVD nitride]] | ||
==Deposition of Silicon Nitride using LPCVD== | |||
[[image:DC_nyhed_3.jpg|320x320px|right|thumb|6" LPCVD nitride furnace (E3) located in cleanroom E-6]] | [[image:DC_nyhed_3.jpg|320x320px|right|thumb|6" LPCVD nitride furnace (E3) located in cleanroom E-6]] | ||
[[image:Furnace_nitride1.jpg|300x300px|right|thumb|4" LPCVD nitride furnace (B2) located in cleanroom B-1]] | [[image:Furnace_nitride1.jpg|300x300px|right|thumb|4" LPCVD nitride furnace (B2) located in cleanroom B-1]] | ||
DTU Nanolab has two LPCVD (Low Pressure Chemical Vapour Deposition) furnaces <!--[[Specific Process Knowledge/Thin film deposition/B2 Furnace LPCVD Nitride|LPCVD furnaces]]--> for deposition of silicon nitride: | DTU Nanolab has two LPCVD (Low Pressure Chemical Vapour Deposition) furnaces <!--[[Specific Process Knowledge/Thin film deposition/B2 Furnace LPCVD Nitride|LPCVD furnaces]]--> for deposition of silicon nitride: | ||
| Line 54: | Line 53: | ||
*[[/Deposition of low stress nitride using the 6" LPCVD nitride furnace|Deposition of low stress nitride using the 6" LPCVD nitride furnace ]] | *[[/Deposition of low stress nitride using the 6" LPCVD nitride furnace|Deposition of low stress nitride using the 6" LPCVD nitride furnace ]] | ||
*[[/Deposition of stoichiometric nitride using the 6" LPCVD nitride furnace|Deposition of stoichiometric nitride using the 6" LPCVD nitride furnace <span style="color:Red">(4" wafers need a special permission)</span>]] | *[[/Deposition of stoichiometric nitride using the 6" LPCVD nitride furnace|Deposition of stoichiometric nitride using the 6" LPCVD nitride furnace <span style="color:Red">(4" wafers need a special permission using as a back up of 4" LPCVD nitride furnace, B2)</span>]] | ||
*[[/Using LPCVD silicon nitride as a masking material for KOH etching|Using LPCVD silicon nitride as a masking material for KOH etching]] | *[[/Using LPCVD silicon nitride as a masking material for KOH etching|Using LPCVD silicon nitride as a masking material for KOH etching]] | ||