Specific Process Knowledge/Wafer cleaning/Post CMP Cleaner: Difference between revisions
Appearance
Created page with "'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Waf..." |
mNo edit summary |
||
| (8 intermediate revisions by 2 users not shown) | |||
| Line 1: | Line 1: | ||
{{cc-nanolab}} | |||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Wafer_cleaning/Post_CMP_Cleaner click here]''' | |||
'''All links to Labmanager requires login.''' | |||
=< | == Post CMP Cleaner) == | ||
[[image:post cmp cleaner.jpg|400px|right|thumb|The Post CMP CLeaner in cleanroom A-5]] | |||
The post CMP Cleaner is designed for removing slurry residues from polishing wafers. The Post CMP cleaner is the recommended cleaning tool after using the '''[http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/Polisher_CMP Polisher CMP]'''. | |||
'''The user manual, user APV, technical information and contact information can be found in LabManager:''' | |||
<!-- remember to remove the type of documents that are not present --> | |||
<!-- give the link to the equipment info page in LabManager: --> | |||
[http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=431 The Post CMP Cleaner in LabManager] | |||
==Equipment performance and process related parameters== | |||
{| border="2" cellspacing="0" cellpadding="2" | |||
!colspan="2" border="none" style="background:silver; color:black;" align="center"|Equipment | |||
|style="background:WhiteSmoke; color:black"|<b>Post CMP Cleaner</b> | |||
<!-- |style="background:WhiteSmoke; color:black"|<b>Equipment 2</b> --> | |||
|- | |||
!style="background:silver; color:black;" align="center" width="60"|Purpose | |||
|style="background:LightGrey; color:black"| | |||
Cleaning of | |||
|style="background:WhiteSmoke; color:black"| | |||
*Samples from the CMP | |||
<!-- |style="background:WhiteSmoke; color:black"| | |||
*Purpose 1 | |||
*Purpose 2 | |||
*Purpose 3 --> | |||
|- | |||
|- | |||
!style="background:silver; color:black" align="center" valign="center" rowspan="4"|Process parameter range | |||
|- | |||
|style="background:LightGrey; color:black"|Mechanical Cleaning | |||
|style="background:WhiteSmoke; color:black"| | |||
*Brush Cleaning | |||
|- | |||
|style="background:LightGrey; color:black"|Power | |||
|style="background:WhiteSmoke; color:black"| | |||
*Megasonic Power from 0-40 W (in water) | |||
|- | |||
|style="background:LightGrey; color:black"|Arm sweep | |||
|style="background:WhiteSmoke; color:black"| | |||
*4" and 6" (20x20mm and 2" run with a 4" sweep) | |||
|- | |||
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Substrates | |||
|style="background:LightGrey; color:black"|Sample size | |||
|style="background:WhiteSmoke; color:black"| | |||
*<nowiki></nowiki> one 20x20mm piece | |||
*one 50 mm wafer | |||
*one 2" wafer | |||
*one 100 mm wafer | |||
*one 150 mm wafer | |||
<!-- |style="background:WhiteSmoke; color:black"| | |||
*<nowiki>#</nowiki> small samples | |||
*<nowiki>#</nowiki> 50 mm wafers | |||
*<nowiki>#</nowiki> 100 mm wafers | |||
*<nowiki>#</nowiki> 150 mm wafers --> | |||
|- | |||
| style="background:LightGrey; color:black"|Allowed materials | |||
|style="background:WhiteSmoke; color:black"| | |||
*Silicon | |||
*Polysilicon | |||
*Silicon Oxide | |||
*Glass/Quartz | |||
<!-- |style="background:WhiteSmoke; color:black"| | |||
*Allowed material 1 | |||
*Allowed material 2 | |||
*Allowed material 3 --> | |||
|- | |||
|} | |||
<br clear="all" /> | |||
Latest revision as of 17:06, 10 June 2025
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here
All links to Labmanager requires login.
Post CMP Cleaner)

The post CMP Cleaner is designed for removing slurry residues from polishing wafers. The Post CMP cleaner is the recommended cleaning tool after using the Polisher CMP.
The user manual, user APV, technical information and contact information can be found in LabManager:
The Post CMP Cleaner in LabManager
| Equipment | Post CMP Cleaner | |
|---|---|---|
| Purpose |
Cleaning of |
|
| Process parameter range | ||
| Mechanical Cleaning |
| |
| Power |
| |
| Arm sweep |
| |
| Substrates | Sample size |
|
| Allowed materials |
| |