Specific Process Knowledge/Thermal Process/Furnace APOX: Difference between revisions
No edit summary |
mNo edit summary |
||
| (40 intermediate revisions by 10 users not shown) | |||
| Line 1: | Line 1: | ||
{{cc-nanolab}} | |||
D1 | '''Feedback to this page''': '''[mailto:thinfilm@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/Furnace_APOX click here]''' | ||
'''<p style="color:red;">The APOX furnace has been decomissioned in August 2019.</span>''' | |||
[[Category: Equipment |Thermal APOX]] | |||
[[Category: Thermal process|APOX]] | |||
[[Category: Furnaces|APOX]] | |||
==Apox furnace (D1)== | |||
[[Image:APOX.JPG|thumb|300x300px|Apox furnace (D1): positioned in the A-5 room/ Photo: DTU Nanolab internal]] | |||
The APOX furnace (D1) is a Tempress horizontal furnace for oxidation silicon wafers. This furnace is dedicated for oxidation of new and clean Si wafers to form apox layers which is a very thick wet thermal oxide grown at 1075<sup>o</sup>C. Running a batch of apox wafers (oxide thickness > 5µm) can take several weeks, depending on how thick an apox layer that is required. | |||
This furnace is positioned in the III-V cleanroom area. Only Nanolab employees are allowed to operate the furnace. | |||
'''The user manual, technical information and contact information can be found in LabManager:''' | |||
'''[http://www.labmanager.dtu.dk/function.php?module=Machine&view=view&mach=159 APOX Furnace (D1)]''' | |||
==Process knowledge== | ==Process knowledge== | ||
| Line 10: | Line 27: | ||
==Overview of the performance of Apox furnace and some process related parameters== | ==Overview of the performance of the Apox furnace and some process related parameters== | ||
{| border="2" cellspacing="0" cellpadding=" | {| border="2" cellspacing="0" cellpadding="2" | ||
|- | |- | ||
!style="background:silver; color:black;" align=" | !style="background:silver; color:black;" align="center"|Purpose | ||
|style="background:LightGrey; color:black"|Oxidation and annealing | |style="background:LightGrey; color:black"| | ||
Oxidation and annealing | |||
|style="background:WhiteSmoke; color:black"|Oxidation: | |style="background:WhiteSmoke; color:black"|Oxidation: | ||
*Wet: | *Wet: With bubbler (water steam + O<sub>2</sub>) | ||
|- | |- | ||
!style="background:silver; color:black" align=" | !style="background:silver; color:black" align="center"|Performance | ||
|style="background:LightGrey; color:black"|Film thickness | |style="background:LightGrey; color:black"|Film thickness | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*Wet | *Wet oxide: Thicker than > 5 µm (APOX layers) | ||
|- | |- | ||
!style="background:silver; color:black" align=" | !style="background:silver; color:black" align="center" valign="center" rowspan="3"|Process parameter range | ||
|style="background:LightGrey; color:black"|Process Temperature | |style="background:LightGrey; color:black"|Process Temperature | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
* | *1075 <sup>o</sup>C | ||
|- | |- | ||
|style="background:LightGrey; color:black"|Process pressure | |style="background:LightGrey; color:black"|Process pressure | ||
| Line 35: | Line 53: | ||
|style="background:LightGrey; color:black"|Gas flows | |style="background:LightGrey; color:black"|Gas flows | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*N< | *N<sub>2</sub>: 0-10 slm | ||
*O<sub>2</sub>: 0-10 slm | |||
|- | |- | ||
!style="background:silver; color:black" align=" | !style="background:silver; color:black" align="center" valign="center" rowspan="2"|Substrates | ||
|style="background:LightGrey; color:black"|Batch size | |style="background:LightGrey; color:black"|Batch size | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
Latest revision as of 14:36, 4 June 2025
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here
The APOX furnace has been decomissioned in August 2019.
Apox furnace (D1)
The APOX furnace (D1) is a Tempress horizontal furnace for oxidation silicon wafers. This furnace is dedicated for oxidation of new and clean Si wafers to form apox layers which is a very thick wet thermal oxide grown at 1075oC. Running a batch of apox wafers (oxide thickness > 5µm) can take several weeks, depending on how thick an apox layer that is required.
This furnace is positioned in the III-V cleanroom area. Only Nanolab employees are allowed to operate the furnace.
The user manual, technical information and contact information can be found in LabManager:
Process knowledge
- Oxidation: look at the Oxidation page
| Purpose |
Oxidation and annealing |
Oxidation:
|
|---|---|---|
| Performance | Film thickness |
|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gas flows |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
|