Jump to content

Specific Process Knowledge/Characterization/Thickness Measurer: Difference between revisions

From LabAdviser
New page: This is a micrometer-screw. It measures with an accurracy within a few µm. Measure the wafer in the box next to the meter.If ok other wafers can be measured. There is a calibration by the...
 
Mmat (talk | contribs)
mNo edit summary
 
(58 intermediate revisions by 9 users not shown)
Line 1: Line 1:
This is a micrometer-screw.
{{cc-nanolab}}
It measures with an accurracy within a few µm.
 
Measure the wafer in the box next to the meter.If ok other wafers can be measured.
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Thickness_Measurer click here]'''
There is a calibration by the DEKTAK.
<br>
It is calibrated at about 750µ
<br>
==Thickness Measurer==
[[Image:Thicknessmeasurer2007.jpg|thumb|300x300px|Thickness Measurer. Positioned in cleanroom D-3]]
 
There are 2 thickness measurers in the cleanroom, both positioned in cleanroom D-3. The Thickness measurer is for measuring all sorts of samples. The thickness measurer (wafers) is solely for measuring the thickness of wafers or depths of grooves on wafers.
 
During a KOH etch it can be helpful to ensure no over-etching by making a thickness measurement during the etching.  
 
 
The user manual, technical information and contact information can be found in
[http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=198 LabManager].
 
==Quality Control - Recipe Parameters and Limits==
{| border="1" cellspacing="2" cellpadding="2" colspan="3"
|bgcolor="#98FB98" |'''Quality Control (QC) for the Thickness measurer'''
|-
|
The measured standard thickness is 0.1 mm. The measured result has to be within &plusmn; 0.005 mm. The QC is preformed once a year.
*[http://www.labmanager.danchip.dtu.dk/d4Show.php?id=1831&mach=198 The QC procedure]<br>
*[https://labmanager.dtu.dk/view_binary.php?type=data&mach=198 The newest QC data]<br>
|}
<br> <br>
 
==Equipment performance and process related parameters==
 
{| border="2" cellspacing="2" cellpadding="3"
 
|-
!style="background:silver; color:black;" align="center"|
Purpose
|style="background:LightGrey; color:black"|
Thickness measurer
|style="background:WhiteSmoke; color:black"|
*Wafer thickness
*Depths of larger grooves
*Heigth of larger samples
|-
!style="background:silver; color:black" align="center"|
Performance
|style="background:LightGrey; color:black"|
Thickness resolution
|style="background:WhiteSmoke; color:black"|
*< 1 µm
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="2"|
Substrates
|style="background:LightGrey; color:black"|
Batch size
|style="background:WhiteSmoke; color:black"|
*One sample
|-
| style="background:LightGrey; color:black"|Substrate materials allowed
|style="background:WhiteSmoke; color:black"|
*No restrictions
|-
|}
<br>
{| border="2" cellspacing="2" cellpadding="3"
 
|-
!style="background:silver; color:black;" align="center"|
Purpose
|style="background:LightGrey; color:black"|
Thickness measurer (wafers)
|style="background:WhiteSmoke; color:black"|
*Wafer thickness
*Depths of larger grooves
|-
!style="background:silver; color:black" align="center"|
Performance
|style="background:LightGrey; color:black"|
Thickness resolution
|style="background:WhiteSmoke; color:black"|
*< 1 µm
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="2"|
Substrates
|style="background:LightGrey; color:black"|
Batch size
|style="background:WhiteSmoke; color:black"|
*One sample
|-
| style="background:LightGrey; color:black"|Substrate materials allowed
|style="background:WhiteSmoke; color:black"|
*Only wafers
|-
|}

Latest revision as of 16:16, 2 June 2025

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here

Thickness Measurer

Thickness Measurer. Positioned in cleanroom D-3

There are 2 thickness measurers in the cleanroom, both positioned in cleanroom D-3. The Thickness measurer is for measuring all sorts of samples. The thickness measurer (wafers) is solely for measuring the thickness of wafers or depths of grooves on wafers.

During a KOH etch it can be helpful to ensure no over-etching by making a thickness measurement during the etching.


The user manual, technical information and contact information can be found in LabManager.

Quality Control - Recipe Parameters and Limits

Quality Control (QC) for the Thickness measurer

The measured standard thickness is 0.1 mm. The measured result has to be within ± 0.005 mm. The QC is preformed once a year.



Equipment performance and process related parameters

Purpose

Thickness measurer

  • Wafer thickness
  • Depths of larger grooves
  • Heigth of larger samples

Performance

Thickness resolution

  • < 1 µm

Substrates

Batch size

  • One sample
Substrate materials allowed
  • No restrictions


Purpose

Thickness measurer (wafers)

  • Wafer thickness
  • Depths of larger grooves

Performance

Thickness resolution

  • < 1 µm

Substrates

Batch size

  • One sample
Substrate materials allowed
  • Only wafers