==Probe Station==
{{cc-nanolab}}


'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Probe Station click here]'''  
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Probe_station click here]'''
<br>
<br>
=Probe Station=
[[Image:probe2.jpg|thumb|300x300px|Probe station. Positioned in serviceroom CX1]]


The Probe station is a - EPS150Triax - Cascade. The purpose is to measure I/V measurement, ohmic measurements etc. It has 4 individually adjustable triax connected probes, but can be fitted with additional coax connected probes. The stage can be moved in x and y to step and repeat a measurement over a large number of chips.


The Four-Point Probe is a Veeco FPP-5000 for I/V measurement. The main purpose is to measure resistance and resistivity on a 4" silicon wafer. But can also be used to find thickness of thin layers or test if is a N- or P-type wafer.  
Samples can be inspected by either a microscope and/or a camera.


The wafer are pushed down on the four pins so a measurement is performed. It works only for 4" wafers because a special holder is need.
Two Keithley 2450 source meters are connected to the probe station by triax cables. An additional Keithley 2410 source meter and a Keithley 2000 multi meter is connected by coax cables. All Keithleys can also be connected with banana wires.
[[Image:probestation.jpg|thumb|300x300px|Probe station: positioned in Service room CX1]]


'''The user manual, technical information and contact information can be found in LabManager:'''


'''[http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=169 Four point probe]'''
The user manual, technical information and contact information can be found in
[http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=343 '''Labmanager]'''.
 
 
==Performance and Process Parameters==
 
{| border="2" cellspacing="2" cellpadding="3"
 
|-
!style="background:silver; color:black;" align="center"|
Purpose
|style="background:LightGrey; color:black"|
Electrical measurements
|style="background:WhiteSmoke; color:black"|
*I/V
*Resistance
*Data collection by PC possible
|-
!style="background:silver; color:black" align="center"|
Performance
|style="background:LightGrey; color:black"|
Pad size
|style="background:WhiteSmoke; color:black"|
*100x100µm or more
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="2"|
Substrates
|style="background:LightGrey; color:black"|
Batch size
|style="background:WhiteSmoke; color:black"|
*One sample
|-
| style="background:LightGrey; color:black"|Substrate materials allowed
|style="background:WhiteSmoke; color:black"|
*No restrictions
|-
|}