==Test of the deposition rate of Silicon and film characteristics==
==Test of the deposition rate of Silicon and film characteristics==
'''''The work in this section was done by Kristian Hagsted Rasmussen @DTU Danchip before 2012 with followup by Berit Herstrøm @DTU Nanolab.'''''
'''''The work in this section was done by Kristian Hagsted Rasmussen @DTU Nanolab (former DTU Danchip) before 2012 - '''''
Please note that it is no longer possible to deposit Si with the Ion beam etcher here at Nanolab.
 
'''''with followup by Berit Herstrøm (bghe) @DTU Nanolab.'''''
 
Please note that it is from 2022 no longer possible to deposit Si with the Ion beam etcher here at Nanolab.