Jump to content

Specific Process Knowledge/Lithography/nLOF: Difference between revisions

Taran (talk | contribs)
Taran (talk | contribs)
 
(One intermediate revision by the same user not shown)
Line 24: Line 24:
*PEB temperature: 110°C
*PEB temperature: 110°C
*PEB time: 60 s
*PEB time: 60 s


The recommended PEB for nLOF is 60 seconds at 110°C, regardless of resist film thickness.
The recommended PEB for nLOF is 60 seconds at 110°C, regardless of resist film thickness.


===PEB baking time investigation===
===PEB baking time investigation===