Jump to content

Specific Process Knowledge/Etch/DRIE-Pegasus/nanobosch/nanobosch6: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
Jmli (talk | contribs)
No edit summary
 
(2 intermediate revisions by the same user not shown)
Line 1: Line 1:
<!--Checked for updates on 10/7-2019 - ok/jmli -->
<!-- Ok, jmli 20170627 -->
<!-- Ok, jmli 20170627 -->
<!-- Ok, jmli 20170627 -->
<!-- Ok, jmli 20170627 -->
<!--Checked for updates on 24/8-2021. ok/ jmli-->
<!--Checked for updates on 4/4-2025 - ok/jmli -->
== Test run using AZ resist 24/9-2012 ==
== Test run using AZ resist 24/9-2012 ==
<!-- revised 1/6-2015 by jmli -->
<!-- revised 1/6-2015 by jmli -->

Latest revision as of 08:35, 4 April 2025


Test run using AZ resist 24/9-2012

Process conditions
Substrate information Wafer C01296.05
Mask Travka50 mask in a few microns of AZ resist
Date 24/9-2012
Tool Pegasus
Process Recipe nanobosch6
Tool conditioning 3 minute TDESC clean
Process duration 15 minutes
Purpose test
Characterisation SEM Zeiss


Test run using AZ resist 24/9-2012

Process conditions
Substrate information Wafer C01296.09
Mask Travka80 mask in a few microns of AZ resist
Date 24/9-2012
Tool Pegasus
Process Recipe nanobosch6
Tool conditioning 3 minute TDESC clean
Process duration 15 minutes
Purpose test