Jump to content

Specific Process Knowledge/Etch/Aluminum Oxide: Difference between revisions

Pevo (talk | contribs)
No edit summary
Mbec (talk | contribs)
No edit summary
 
(3 intermediate revisions by one other user not shown)
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Aluminum_Oxide click here]'''
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.'''
 
'''All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.'''
 
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Aluminum_Oxide click here]'''


Etching Al<sub>2</sub>O<sub>3</sub> can be done both chemically (wet) and by dry etching.  
Etching Al<sub>2</sub>O<sub>3</sub> can be done both chemically (wet) and by dry etching.  
Chemical etching can be done using HF or a developer. The last has not been tested. This will be selective to most materials not containing Al. Do expect a slow and isotropic etch rate of about 1-2 nm/min.  
Chemical etching can be done using BHF (60nm/min) or a developer (4nm/min). This will be selective to most materials not containing Al.  
We have done some test of Al<sub>2</sub>O<sub>3</sub> in dry etching. It has been mostly tested in the III-V ICP and ICP Metal. Please see links below.
We have done some test of Al<sub>2</sub>O<sub>3</sub> in dry etching. It has been mostly tested in the III-V ICP and ICP Metal. Please see links below.