Jump to content

Specific Process Knowledge/Etch/Aluminum Oxide: Difference between revisions

Bghe (talk | contribs)
No edit summary
Mbec (talk | contribs)
No edit summary
 
(10 intermediate revisions by 4 users not shown)
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Aluminum_Oxide click here]'''
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.'''


'''All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.'''


=<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>[[image:Under_construction.png|200px]]=
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Aluminum_Oxide click here]'''


Etching Al<sub>2</sub>O<sub>3</sub> can be done both chemically (wet) and by dry etching.
Chemical etching can be done using BHF (60nm/min) or a developer (4nm/min). This will be selective to most materials not containing Al.
We have done some test of Al<sub>2</sub>O<sub>3</sub> in dry etching. It has been mostly tested in the III-V ICP and ICP Metal. Please see links below.


*[[/Al2O3 Etch with ICP Metal|Al2O3 etch using ICP metal]]
 
*[[/Al2O3 Etch with ICP Metal|Al<sub>2</sub>O<sub>3</sub> etch using ICP metal]]
*[[/Al2O3 Etch with III-V ICP|Al<sub>2</sub>O<sub>3</sub> etch using III-V ICP]]
*[[/Al2O3 Etch using HF|Al<sub>2</sub>O<sub>3</sub> etch using HF]]