Specific Process Knowledge/Etch/Etching of Titanium: Difference between revisions
Appearance
No edit summary |
|||
| (17 intermediate revisions by 5 users not shown) | |||
| Line 1: | Line 1: | ||
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.''' | |||
'''All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.''' | |||
'''Feedback to this page''': '''[mailto:labadviser@ | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Etching_of_Titanium click here]''' | ||
<!--Page reviewed by jmli 1/8-2016 --> | |||
==Etching of Titanium== | ==Etching of Titanium== | ||
| Line 12: | Line 13: | ||
<br clear="all" /> | <br clear="all" /> | ||
==Comparison of | ==Comparison of Titanium Etch Methodes== | ||
{|border="1" cellspacing="1" cellpadding="3" style="text-align:left;" | {|border="1" cellspacing="1" cellpadding="3" style="text-align:left;" | ||
| Line 20: | Line 21: | ||
|-style="background:silver; color:black" | |-style="background:silver; color:black" | ||
! | ! | ||
![[Specific Process Knowledge/Etch/Wet | ![[Specific Process Knowledge/Etch/Wet Titanium Etch|Ti wet etch 1]] | ||
![[Specific Process Knowledge/Etch/Wet | ![[Specific Process Knowledge/Etch/Wet Titanium Etch|Ti wet etch 2]] | ||
![[Specific_Process_Knowledge/Etch/ICP_Metal_Etcher|ICP metal]] | ![[Specific_Process_Knowledge/Etch/ICP_Metal_Etcher|ICP metal]] | ||
![[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE (Ionfab300+)]] | ![[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE (Ionfab300+)]] | ||
| Line 29: | Line 30: | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
!Generel description | !Generel description | ||
| | |BHF Etch of titanium with or without photoresist mask. | ||
| | |Cold RCA1 mix etch of titanium (as stripper or with eagle resist). | ||
|Dry plasma etch of | |Dry plasma etch of Ti | ||
|Sputtering of | |Sputtering of Ti - pure physical etch | ||
|- | |- | ||
| Line 39: | Line 40: | ||
!Etch rate range | !Etch rate range | ||
| | | | ||
*~ | *~?nm/min | ||
| | | | ||
*~?nm/min | *~?nm/min | ||
| | | | ||
*~ | *~50-200 nm/min (depending on features size and etch load and recipe settings) | ||
| | | | ||
*~ | *~20nm/min | ||
|- | |- | ||
| Line 71: | Line 72: | ||
| | | | ||
*smaller pieces on a carrier wafer | *smaller pieces on a carrier wafer | ||
*<nowiki>#</nowiki>1 100mm wafers ( | *<nowiki>#</nowiki>1 100mm wafers (if you place it/bond it on a 150 mm carrier wafer) | ||
*<nowiki>#</nowiki>1 150mm wafers | *<nowiki>#</nowiki>1 150mm wafers | ||
| | | | ||
Smaller pieces glued to carrier wafer | Smaller pieces glued to carrier wafer | ||
| Line 114: | Line 115: | ||
|} | |} | ||