Specific Process Knowledge/Thin film deposition/Gadolinium Cerium Oxide: Difference between revisions
Appearance
Created page with "'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Gadolinium_Cerium_Oxide click here]''' ''All text by Nanolab staff'' <br clear="all" /> == Deposition of Gadolinium Cerium Oxide == Thin films of Gadolinium Cerium Oxide (Gd<sub>0.2</sub>Ce<sub>0.8</sub>O<sub>2</sub>) can be deposited using RF sputtering. In this process, the ma..." |
|||
| Line 35: | Line 35: | ||
!Stoichiometry | !Stoichiometry | ||
| | | | ||
* | *Gd<sub>0.2</sub>Ce<sub>0.8</sub>O<sub>2</sub> (can be tuned) | ||
|- | |- | ||
| Line 64: | Line 64: | ||
!Process Temperature | !Process Temperature | ||
| | | | ||
* Up to | * Up to 600 °C (most likely in the range of 200°C) | ||
|- | |- | ||
Latest revision as of 18:46, 7 February 2024
Feedback to this page: click here
All text by Nanolab staff
Deposition of Gadolinium Cerium Oxide
Thin films of Gadolinium Cerium Oxide (Gd0.2Ce0.8O2) can be deposited using RF sputtering. In this process, the main parameters are temperature and additional oxygen, which can be adjusted to tailor the properties of the deposited films. The target is a solid ceramic 75 mm (0.125" thickness) GCO target bonded to a Cu plate.
GCO sputtering in Sputter-System Metal-Oxide (PC1)
| Sputter-System Metal-Oxide (PC1)/Sputter-System Metal-Nitride (PC3) | |
|---|---|
| Generel description |
|
| Stoichiometry |
|
| Film Thickness |
|
| Deposition rate |
|
| Step coverage |
|
| Process Temperature |
|
| Substrate size |
|
| Allowed materials |
|