=Beamer guide= | =Beamer guide= | ||
| Line 6: | Line 8: | ||
For a more in depth look at Beamer please refer to GenISys own [https://www.genisys-gmbh.com/in-action.html learning material found here.] | For a more in depth look at Beamer please refer to GenISys own [https://www.genisys-gmbh.com/in-action.html learning material found here.] | ||
Currently the content below is a mix of Beamer 6 and 7, we are working towards changing it all to Beamer 7. The difference is mostly visual though. | |||
==Beamer nodes== | ==Beamer nodes== | ||
| Line 321: | Line 327: | ||
===Visual-Job=== | ===Visual-Job=== | ||
Visual Job is essentially a graphical interface where one can setup a job consisting of multiple patterns. After setup Visual Job vil write the corresponding SDF and JDF files. A short video guide to | Visual Job is essentially a graphical interface where one can setup a job consisting of multiple patterns. After setup Visual Job vil write the corresponding SDF and JDF files. A short video guide to [https://youtu.be/Mi_HimB0Xa8?si=7WemvXTKJMGLY2jb Visual Job is available here.] Notice that the video is from Beamer 6.2, there is only a few minor changes in Beamer 7. | ||
===PEC=== | ===PEC=== | ||