==Correct settings for temperatures on Pegasus 2 ==
==Correct settings for temperatures on Pegasus 2 ==


The Platen chiller temperature is enabled and the setpoint is 20 degrees. This setting could be applied to all the heaters, however, the best way by far is to run the processes without enabling  
The Platen chiller temperature is enabled and the setpoint is 20 degrees as seen in the image below. This setting could be applied to all the heaters, however, the best way by far is to run the processes without enabling the heaters as seen for the other heaters.


[[file:Peg2tempsettings.jpg | 400px | frameless]]
[[file:Peg2tempsettings.jpg | 400px | frameless]]

Revision as of 11:50, 28 June 2023

Feedback to this page: click here


Unless otherwise stated, the content of this page was created by the dry etch group at DTU Nanolab

Correct settings for temperatures on Pegasus 2

The Platen chiller temperature is enabled and the setpoint is 20 degrees as seen in the image below. This setting could be applied to all the heaters, however, the best way by far is to run the processes without enabling the heaters as seen for the other heaters.