'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.labadviser.dtu.dk/index.php/Sputtering_of_Ti_in_Wordentec click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.labadviser.dtu.dk/index.php/Sputtering_of_Ti_in_Wordentec click here]''' | ||
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i> | |||
== Deposition rate == | == Deposition rate == |
Latest revision as of 10:35, 11 May 2023
Feedback to this page: click here
Unless otherwise stated, this page is written by DTU Nanolab internal
Deposition rate
The deposition rate will change with the settings for pressure and power.
Pressure: 1*10-2 mbar, Power: 300 W
The rate in the Wordentec is established to be 1.7 Å/s (in the centre of the wafer, 1.3 Å/s at the edge) (data from before 2018).