'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.labadviser.dtu.dk/index.php/Sputtering_of_Ti_in_Wordentec click here]'''
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i>
== Deposition rate ==
== Deposition rate ==


The deposition rate will change with the settings for pressure and effect.   
The deposition rate will change with the settings for pressure and power.   




'''Pressure <math>1*10^{-2}</math> mbar, Effect 300 W'''
'''Pressure: 1*10<sup>-2</sup> mbar, Power: 300 W'''


The rate is established to be 1.7 Å/s (in the center of the wafer, 1.3 Å/s at the edge).
The rate in the [[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec]] is established to be 1.7 Å/s (in the centre of the wafer, 1.3 Å/s at the edge) (data from before 2018).

Latest revision as of 10:35, 11 May 2023

Feedback to this page: click here

Unless otherwise stated, this page is written by DTU Nanolab internal

Deposition rate

The deposition rate will change with the settings for pressure and power.


Pressure: 1*10-2 mbar, Power: 300 W

The rate in the Wordentec is established to be 1.7 Å/s (in the centre of the wafer, 1.3 Å/s at the edge) (data from before 2018).