Specific Process Knowledge/Etch/Etching of Chromium: Difference between revisions
Appearance
No edit summary |
|||
| (One intermediate revision by one other user not shown) | |||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@ | '''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.''' | ||
'''All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.''' | |||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Etching_of_Chromium click here]''' | |||
<!--Page reviewed by jmli 1/8-2016 --> | <!--Page reviewed by jmli 1/8-2016 --> | ||
<!--Page reviewed by jmli 9/8-2022 --> | |||
==Etching of Chromium== | ==Etching of Chromium== | ||
| Line 72: | Line 79: | ||
|- | |- | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
! | !Allowed materials | ||
| | | | ||
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals | No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals | ||
Latest revision as of 15:47, 6 February 2023
Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.
All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.
Feedback to this page: click here
Etching of Chromium
Etching of chromium can be done either by wet etch, dry etch or by sputtering with ions.
Comparison of Chromium Etch Methods
| Cr wet etch | ICP metal | IBE (Ionfab300+) | |
|---|---|---|---|
| Generel description | Wet etch of Cr premixed (Chrome etch 18) | Dry plasma etch of Cr | Sputtering of Cr - pure physical etch |
| Etch rate range |
|
|
|
| Etch profile |
|
|
|
| Substrate size |
|
|
Smaller pieces glued to carrier wafer
|
| Allowed materials |
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals |
|
|