Specific Process Knowledge/Lithography/mrEBL6000: Difference between revisions
Appearance
No edit summary |
mNo edit summary |
||
| (2 intermediate revisions by the same user not shown) | |||
| Line 3: | Line 3: | ||
mrEBL6000 works as a negative e-beam resist but is also UV sensitive, why resist and coated wafers should be kept in yellow rooms only. When carrying the wafers to the e-beam writer, use a black or blue box for protection. While mounting the wafers in the e-beam cassettes, you can turn off the white light in the e-beam room and turn on the yellow light which is located above the pre-aligner setup. | mrEBL6000 works as a negative e-beam resist but is also UV sensitive, why resist and coated wafers should be kept in yellow rooms only. When carrying the wafers to the e-beam writer, use a black or blue box for protection. While mounting the wafers in the e-beam cassettes, you can turn off the white light in the e-beam room and turn on the yellow light which is located above the pre-aligner setup. Please mount as close to exposure as possible and turn of the with light outside the room and place a note on the door not to turn on light while the cassette is in the stocker. | ||
mrEBL6000 is a chemically amplified | mrEBL6000 is a chemically amplified resist, i.e. immediately after e-beam exposure, the wafers require a post-exposure bake. If no post-exposure bake is performed, the resist is not crosslinked and will most likely dissolve during development. | ||
This resist can be used as standard negative resist at Nanolab, but due to limited use, we often need to buy a new bottle, hence please ask long time (up to 3 months) in advance for this chemical. or by it yourself! | |||
<br> | <br> | ||
<br> | <br> | ||