8 September 2026

  • curprev 09:5409:54, 8 September 2026 Mmat talk contribs 1,772 bytes +1,772 Created page with "thumb|470x470px|The Nanoscribe Quantum X align in PolyFabLab. == Introduction == The Nanoscribe Quantum X align is a 3D printer based on two-photon polymerization (2PP) and designed for rapid microfabrication of polymer structures. It features a femtosecond pulsed diode laser operating at 780 nm outputting a laser power of 250 mW. In addition, it is equipped with a sample stage with a 50 × 50 × 20 mm travel range that can fit up to an 8-in..."