Jump to content

Specific Process Knowledge/Lithography/Descum/plasmaAsher03: Revision history

Diff selection: Mark the radio buttons of the revisions to compare and hit enter or the button at the bottom.
Legend: (cur) = difference with latest revision, (prev) = difference with preceding revision, m = minor edit.

12 January 2026

  • curprev 12:1312:13, 12 January 2026 Jehem talk contribs 2,575 bytes +2,575 Created page with "=Plasma Asher 3: Descum= Product name: Diener Pico Plasma Asher<br> Year of purchase: 2014 The user manual(s), quality control procedure(s) and results and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=423 LabManager] - '''requires login''' Plasma Asher 3 is specifically used for controlled descum process after lithography. Please note that you only can process a single 100 mm wafer, or one small sample, at a t..."